MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow DS6D21 Polypropylene Random Copolymer Resin  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer; Polypropylene, Film Grade

Material Notes:
    Overview
  • Consistent processability
  • High clarity and gloss
  • Complies with U.S. FDA 21 CFR 177.1520 (c)3.1a

DOW DS6D21 Polypropylene Resin is intended for use in case film processes. It is particularly suited for applications requiring high clarity.

Former Dow grade acquired by Braskem.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D792
Melt Index of Compound 8.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 25.0 MPa3630 psiASTM D638
Elongation at Yield 10 %10 %ASTM D638
Flexural Modulus, 1% Secant 758 MPa110000 psiASTM D790A
Izod Impact, Notched 0.480 J/cm0.899 ft-lb/inASTM D256A
 
Thermal PropertiesMetricEnglishComments
Melting Point 142 °C288 °FDSC; Dow Method
Deflection Temperature at 0.46 MPa (66 psi) 81.1 °C178 °FUnannealed; ASTM D648
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow R131-02A Polypropylene Random Copolymer Resin
Dow DS6D82 Polypropylene Random Copolymer Resin
Borealis BA11CF Polypropylene Copolymer
Borealis BD212CF Polypropylene Copolymer
Braskem CP 401 HC Injection Molding Polypropylene

PDOW0968 / 93304

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.