MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik Trogamid® AX9761 Transparent Polyamide  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: TROGAMID AX9761 is an amorphous and transparent polyamide with a glass transition temperature of 135 °C and a light transmission of more than 85%, suitable for injection molding and extrusion. Listings: TROGAMID AX9761 have been approved for direct contact with foodstuffs by the European Community (Directive 90/128/EEC) and the Food and Drug Administration (FDA – 21stCFR, Section 177.1500 Nylon Resins).

Information provided by degussa.

Evonik Industries is the successor company to Degussa.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³ISO 1183
Water Absorption at Saturation 7.8 %7.8 %ISO 62
Viscosity Measurement 1.45 - 1.851.45 - 1.85Relative Solution Viscosity (m-Cresol); ISO 307
Linear Mold Shrinkage 0.0040 cm/cm0.0040 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0050 cm/cm0.0050 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8888ISO 868
Ball Indentation Hardness 165 MPa23900 psiH30; ISO 2039-1
Tensile Strength, Yield 100 MPa14500 psiISO 527-1/2
Elongation at Break >= 50 %>= 50 %ISO 527-1/2
Elongation at Yield 7.0 %7.0 %ISO 527-1/2
 8.5 %8.5 %Outer fiber strain at maximum stress; ISO 178
Tensile Modulus 2.70 GPa392 ksiISO 527-1/-2
Flexural Strength 85.0 MPa12300 psiat 3.5% strain; ISO 178
 130 MPa18900 psiISO 178
Flexural Modulus 3.30 GPa479 ksiISO 178
Izod Impact, Notched (ISO)  1.10 kJ/m²
@Temperature -30.0 °C
0.523 ft-lb/in²
@Temperature -22.0 °F
ISO 180/1A
 1.20 kJ/m²
@Temperature 0.000 °C
0.571 ft-lb/in²
@Temperature 32.0 °F
ISO 180/1A
 1.20 kJ/m²
@Temperature 23.0 °C
0.571 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
Izod Impact, Unnotched (ISO) NBNBISO 180/1U
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 180/1U
 NB
@Temperature 0.000 °C
NB
@Temperature 32.0 °F
ISO 180/1U
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 125 °C257 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 110 °C230 °FISO 75-1/-2
Vicat Softening Point 130 °C266 °FMethod B, 50 N; ISO 306
 135 °C275 °FMethod A, 10 N; ISO 306
Glass Transition Temp, Tg 135 °C275 °F2nd heating; DSC-7
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %transparent; thickness not quantified
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik Trogamid® A4000 Transparent Polyamide
Evonik Trogamid® CX7323 Transparent Nylon
Evonik Trogamid® T5000 Nylon 6-3
Evonik Trogamid® CX9710 Transparent Nylon
Evonik Trogamid® CX9701 Transparent Nylon

PHUK112 / 47246

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.