MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Erbslöh Aluminium DISPAL S691 Aluminum Alloy, AlCu5Ti
Categories: Metal; Nonferrous Metal; Aluminum Alloy

Material Notes: High stiffness and elongation at rupture

Information provided by PEAK Werkstoff GmbH, a part of Erbslöh Aluminium GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.80 g/cc0.101 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 500 - 540 MPa72500 - 78300 psiafter heat treatment
Tensile Strength, Yield 350 - 460 MPa
@Strain 0.2 %
50800 - 66700 psi
@Strain 0.2 %
after heat treatment
Elongation at Break 10 - 20 %10 - 20 %after heat treatment
Modulus of Elasticity 75.0 GPa10900 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear 23.0 µm/m-°C12.8 µin/in-°F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 94 %94 %As Balance
Copper, Cu 5.0 %5.0 %
Titanium, Ti 1.0 %1.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Erbslöh Aluminium DISPAL S220 Aluminum Alloy, AlSi35, Condition O
Erbslöh Aluminium DISPAL S693 Aluminum Alloy, AlCu5Ti, Condition T4
Erbslöh Aluminium DISPAL S690 Aluminum Alloy, AlCu4MgAg, Condition T4
Erbslöh Aluminium DISPAL S690 Aluminum Alloy, AlCu4MgAg, Condition T6
Erbslöh Aluminium DISPAL S541 Aluminum Alloy, AlMg6Mn4SiTiZr, Condition F

NPEAK08 / 101613

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.