MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

US Plastic Lumber Carefee Xteriors Composite Plastic Lumber  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Wood and Natural Products; Wood

Material Notes: Description: USPL's Composite products are composed of approximately 65% recycled wood/natural fiber and 35% recycled plastic, with selected process additives. The plastic raw material utilized in this product is recycled plastic. It is processed to a uniform feedstock, compounded with recovered fibers and extruded into a rigid board product. USPL Composite boards have many beneficial properties for decking applications, including:
  • Low moisture absorption
  • No rotting, splitting or splintering
  • Inherent termite and UV resistance
  • Excellent dimensional stability and wet/dry traction
  • No toxic compounds (CCA) to leach into soil or groundwater
  • Workability and appearance of natural lumber products.

Applications: USPL Composite E-board 5/4x6 and 2x6 boards are designed for deck, porch, boardwalk, dock and similar applications. These boards may also be used for many lumber applications, where a non-load bearing member is required. This material is particularly well suited for outdoor uses due to its durability characteristics.

Information provided by U.S. Plastic Lumber (USPL).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption 1.66 %1.66 %ASTM D1037
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 5.38 MPa780 psiASTM D198
Modulus of Elasticity 1.52 GPa220 ksiASTM D6109
 2.00 GPa290 ksiASTM D4761
Modulus of Rupture 0.0117 GPa1.70 ksiUltimate; ASTM D4761 & ASTM D6109
Compressive Strength 15.9 MPa2300 psiCompression Parallel and Perpendicular to Grain; ASTM D198
Shear Strength 6.21 MPa900 psiASTM D143
Coefficient of Friction, Static 0.800.80Wet or Dry; Tribometer
 
Thermal PropertiesMetricEnglishComments
CTE, linear 81.0 µm/m-°C
@Temperature 20.0 °C
45.0 µin/in-°F
@Temperature 68.0 °F
ASTM E228
Flame Spread Index 7676ASTM 684
Flash Point 381 °C718 °FFlash-Ignition Temperature; ASTM D1929
 387 °C729 °FSelf-Ignition Temperature; ASTM D1929
 
Descriptive Properties
Nail Withdrawal190 lbs/inASTM D1761 (3.5" x .131")
Screw Withdrawal650 lbs/inASTM D1761

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
American Pine Wood
Medial Collateral Ankle Ligament
Plywood
CHT Group EP Primer 28 EPI Engineered Polymers Aromatic polyisocyanate Prepolymer
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade

PUSPL2 / 71802

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.