MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ashley Polymers Ashlene® 528LSB2-20G Nylon 66, 20% Glass Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 20% Glass Fiber Filled

Material Notes: A UV Stabilized 20% glass fiber reinforced Nylon 66 designed for parts requiring excellent thermal and dimensional stability and higher strength than conventional resins.

Data provided by the manufacturer

Key Words: Polyamide 66; Ashley Polymers, Inc.
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.28 g/cc0.0462 lb/in³ASTM D792
Water Absorption 1.1 %1.1 %24 hrs; ASTM D570
Linear Mold Shrinkage 0.0050 cm/cm0.0050 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 120120ASTM D785
Tensile Strength, Yield 90.0 MPa13100 psiASTM D638
Elongation at Yield 3.0 %3.0 %ASTM D638
Flexural Modulus 4.80 GPa696 ksiASTM D790
Izod Impact, Notched 0.640 J/cm1.20 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 252 °C486 °FASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 249 °C480 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 243 °C469 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ashley Polymers Ashlene® 525LD-13G Nylon 66, 13% Glass Reinforced
Ashley Polymers Ashlene® 527LD-14G Nylon 66, 14% Glass Reinforced
Ashley Polymers Ashlene® 742L-13G Nylon 6/66, 13% Glass Reinforced
Plastcom SLOVAMID 6 NG GF 15 HI PA6, 15% glass fibre, improved strength
Polyram PlusTek PA840G13 Nylon 66 for Injection Molding, 13% Glass Fiber Reinforced, Impact Modified, Heat Resistant

PNAA32 / 54379

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.