MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Aclo Accutech Polypropylene Copolymer CP0437G20CL Glass Reinforced Coupled
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Glass Fiber Filler

Material Notes:

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.01 g/cc0.0365 lb/in³ASTM D792
Linear Mold Shrinkage 0.0010 cm/cm0.0010 in/inMD; ASTM D955
Melt Flow 13 g/10 min13 g/10 minASTM D1238
Ash 20 %20 %ASTM D2584
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 8080ASTM D785
Tensile Strength at Break 40.0 MPa5800 psiASTM D638
Tensile Strength, Yield 42.0 MPa6090 psiASTM D638
Elongation at Break 8.0 %8.0 %ASTM D638
Elongation at Yield 5.0 %5.0 %ASTM D638
Tensile Modulus 2.499 GPa362.5 ksiASTM D638
Flexural Strength 57.0 MPa8270 psiASTM D790
Flexural Modulus 2.80 GPa406 ksiASTM D790
Izod Impact, Notched 1.33 J/cm2.50 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 152 °C306 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 116 °C241 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polypropylene with 20% Glass Fiber Filler
A. Schulman PP 3457-01 Copolymer Polypropylene
A. Schulman POLYFLAM™ FPP 1007 Talc Filled Homopolymer Polypropylene
Aclo Accutech Polypropylene Copolymer CP0437G10CL Glass Reinforced Coupled
Aclo Accutech Polypropylene Homopolymer HP0334T40L1 Talc Reinforced

PACLO148 / 22403

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.