MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

California Fine Wire Stablohm 675 Nickel, Chromium and Iron Resistance Wire
Categories: Metal; Electronic/Magnetic Alloy; Nonferrous Metal; Nickel Alloy

Material Notes: All values may vary dependent on specific design and usage

Capabilities:

  • Wire
  • Ribbon
  • Square
  • Insulated
  • Plated

Information provided by California Fine Wire.

Key Words: ASTM B267, ASTM B344
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.25 g/cc0.298 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 655 MPa95000 psiAnnealed
 1070 MPa155000 psiStress relieved
 1210 MPa175000 psiHard
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000112 ohm-cm0.000112 ohm-cm3% tolerance on sizes below 0.02, 5% tolerance on sizes above 0.02
 
Thermal PropertiesMetricEnglishComments
CTE, linear 14.0 µm/m-°C
@Temperature 20.0 °C
7.78 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 13.2 W/m-K91.6 BTU-in/hr-ft²-°F
Melting Point 1350 °C2462 °F
Maximum Service Temperature, Air 900 °C1650 °FOperating Temperature
 
Component Elements PropertiesMetricEnglishComments
Chromium, Cr 16 %16 %
Iron, Fe 24 %24 %as balance
Nickel, Ni 60 %60 %
 
Descriptive Properties
MagneticFaint
Temperature Coefficient of Resistance0.00015 ohms/ohm-°C0-100°C
Thermal EMF vs. Copper+0.002

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Nickel-Chromium-silicon Iron, heat-resistant gray iron
California Fine Wire Stablohm 610 Nickel, Chromium and Iron Resistance Wire
Alloy 19® Thermocouple Alloy
Haynes Hastelloy® C-22® alloy, 0.71-3.2 mm thick sheet, solution heat treated
Alliance A-5 Alnico Magnetic Material

NCALZ31 / 15574

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.