MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik DYNAPOL® S 320 Linear Copolyester
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: A saturated linear copolyester, moderately crystalline. Generally used for biodegradable adhesives.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity  3000 cP
@Temperature 200 °C
3000 cP
@Temperature 392 °F
melt; (Plate/Plate)
 5000 cP
@Temperature 180 °C
5000 cP
@Temperature 356 °F
melt; (Plate/Plate)
 10000 cP
@Temperature 160 °C
10000 cP
@Temperature 320 °F
melt; (Plate/Plate)
Viscosity Test 80 cm³/g0.80 dl/gDIN 53 728
Melt Flow  240 g/10 min
@Temperature 160 °C
240 g/10 min
@Temperature 320 °F
DIN ISO 1133
 500 g/10 min
@Temperature 180 °C
500 g/10 min
@Temperature 356 °F
DIN ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 3232
 
Thermal PropertiesMetricEnglishComments
Melting Point 100 °C212 °FDIN 53 765
Softening Point 120 °C248 °FDIN ISO 4625
Glass Transition Temp, Tg -40.0 °C-40.0 °FDIN 53 765

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sumitomo Bakelite Durez®-ter S105-30 Polyester Polyol
Evonik DYNAPOL® S 1402 Linear Copolyester

PHUMB280 / 81282

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.