MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical LB100M PVC
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: General Description: LB100M, blend resin exhibits the following characteristics. Reduced viscosity, aging of plastisol, low gloss at the top layers and improved deaeration of plastically

Main Applications: Reducing plastically viscosity, low gloss, good mat effect.

CAS No: 9002-86-2

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.406 g/cc1.406 g/cc
Molecular Weight 60000 - 150000 g/mol60000 - 150000 g/mol
 
Thermal PropertiesMetricEnglishComments
Melting Point 302 °C576 °F
Ignition Temperature 435 °C815 °FAutoignition

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical LP170 PVC
LG Chemical HF380NS ABS, High Flow, General Anti-Static
LG Chemical AT-553 Transparent ABS, Permanent Antistatic, Natural and Colored Pellets
LG Chemical PI642G ABS, General Purpose, High Modulus
LG Chemical LUPOS HR2207A ABS+GF20%, General Purpose, Heat Resistance

PLAY722 / 148732

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.