MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Meldin Supplier

DuPont Mobility and Materials VESPEL TP-8311 Polyimide
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic

Material Notes: Thermoplastic parts from filled PI (polyimide) for balanced mechanical properties and low wear and friction performance in both dry and lubricated high temperature environments

Information provided by DuPont. This product line has remained with DuPont after the DuPont-Dow merger.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.38 g/cc1.38 g/ccASTM D792
 1.38 g/cc
@Temperature 23.0 °C
1.38 g/cc
@Temperature 73.4 °F
ASTM D792
Water Absorption 0.11 %
@Temperature 23.0 °C
0.11 %
@Temperature 73.4 °F
Immersion 24h; ASTM D570
Moisture Absorption 0.11 %
@Temperature 23.0 °C
0.11 %
@Temperature 73.4 °F
50%RH,23°C,24h; ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break 4.0 %
@Temperature 23.0 °C
4.0 %
@Temperature 73.4 °F
ASTM D638
Flexural Strength 215 MPa
@Temperature 23.0 °C
31200 psi
@Temperature 73.4 °F
ASTM D790
Flexural Modulus 6.30 GPa
@Temperature 23.0 °C
914 ksi
@Temperature 73.4 °F
ASTM D790
Compressive Strength 44.0 MPa
@Temperature 23.0 °C
6380 psi
@Temperature 73.4 °F
ASTM D695
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 17.0 µm/m-°C
@Temperature 23.0 - 150 °C
9.44 µin/in-°F
@Temperature 73.4 - 302 °F
ASTM E 228
CTE, linear, Transverse to Flow 50.0 µm/m-°C
@Temperature 23.0 - 150 °C
27.8 µin/in-°F
@Temperature 73.4 - 302 °F
ASTM E 228
Glass Transition Temp, Tg 249 °C480 °FASTM D3418
UL RTI, Electrical  50.0 °C
@Thickness 0.750 mm
122 °F
@Thickness 0.0295 in
UL 746B
 50.0 °C
@Thickness 1.50 mm
122 °F
@Thickness 0.0591 in
UL 746B
 50.0 °C
@Thickness 3.00 mm
122 °F
@Thickness 0.118 in
UL 746B
UL RTI, Mechanical with Impact  50.0 °C
@Thickness 1.50 mm
122 °F
@Thickness 0.0591 in
UL 746B
 50.0 °C
@Thickness 3.00 mm
122 °F
@Thickness 0.118 in
UL 746B
 50.0 °C
@Thickness 0.750 mm
122 °F
@Thickness 0.0295 in
UL 746B
UL RTI, Mechanical without Impact  50.0 °C
@Thickness 0.750 mm
122 °F
@Thickness 0.0295 in
UL 746B
 50.0 °C
@Thickness 1.50 mm
122 °F
@Thickness 0.0591 in
UL 746B
 50.0 °C
@Thickness 3.00 mm
122 °F
@Thickness 0.118 in
UL 746B
Flammability, UL94  V-0
@Thickness 0.750 mm
V-0
@Thickness 0.0295 in
IEC 60695-11-10
 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
IEC 60695-11-10
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
IEC 60695-11-10
 V-0
@Thickness 0.750 mm
V-0
@Thickness 0.0295 in
UL94
 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
UL94
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
UL94
 
Descriptive Properties
AppearanceNatural Color
FormsShapes
Heat StabilizedYes
Material StatusCurrent
Polymer FamilyPolyimide
Polymer TypePI
Region Available - GlobalYes
Ultrasonic WeldableYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
G-10 Fiberglass Epoxy Laminate Sheet
Ensinger TECAPEI® 10% Glass Reinforced, made from Ultem® 2100 PEI
DuPont Mobility and Materials VESPEL TP-8054 Polyimide
DuPont Mobility and Materials VESPEL TP-8169 Polyimide
DuPont Mobility and Materials VESPEL TP-8212 Polyimide

PDSZ1274 / 140091

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.