MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Changzhou Jinlibao GETAILONG JLB-110800 APET Sheet
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes:

Information provided by Changzhou Jinlibao Plastic Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 20.0 - 15000 microns0.787 - 591 mil
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 60.0 MPa
@Thickness 1.00 mm
8700 psi
@Thickness 0.0394 in
Elongation at Break >= 65 %>= 65 %
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.210 W/m-K1.46 BTU-in/hr-ft²-°F
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 80 - 95 %80 - 95 %
 
Descriptive Properties
ColorClear, White, Green, Blue, Orange, Brown

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
American Computer Optics UV Protection Glass 2 mm
American Computer Optics 10.4in Tempered LCD Glass
Aluminum 5657-H25
Aluminum 5052-H32
Changzhou Jinlibao GETAILONG JLB-110900 Clear PETG sheet

PCHANG001 / 184977

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.