MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Metflex EM85 Natural Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Natural rubber compound developed specifically for subsea and offshore applications. Material properties formulated with very high tensile properties, resilience and dynamic properties with very good resistance to ageing when exposed to heat build-up in service. Tear and abrasion resistance is also better than most synthetic elastomers.

Information provided by Metflex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.28 g/cc1.28 g/ccISO 2781
Water Absorption <= 1.0 %
@Temperature 23.0 °C
<= 1.0 %
@Temperature 73.4 °F
2 weeks; ISO 1817
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8484IRHD; ISO 48
Tensile Strength 16.0 MPa2320 psiISO 37: Type 2
Elongation at Break 230 %230 %ISO 37: Type 2
Compressive Modulus 0.00113 GPa
@Strain 30 %
0.164 ksi
@Strain 30 %
ISO 7743
Rebound 26 %26 %Rebound Resilience; ASTM D2632
Shear Modulus  0.00230 GPa
@Strain 40 %
0.334 ksi
@Strain 40 %
ISO 1827
 0.00270 GPa
@Strain 25 %
0.392 ksi
@Strain 25 %
ISO 1827
Compression Set 9.0 %
@Temperature 22.0 °C,
Time 259000 sec
9.0 %
@Temperature 71.6 °F,
Time 72.0 hour
25% strain; ISO 815
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 70.0 °C158 °F
Minimum Service Temperature, Air -50.0 °C-58.0 °F
 
Descriptive Properties
Stress Relaxation Rate3.4%25% @ 22°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Metflex EM67 Natural Rubber
Metflex EM73 Natural Rubber
Metflex EM78 Natural Rubber
Natural Rubber, Vulcanized (NR, IR, Polyisoprene)
Natural Rubber, Not Vulcanized (NR, IR, Polyisoprene)

PMETF008 / 197392

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.