MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Teijin Films Melinex® 542 Polyester Film
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Melinex® 542 is a slightly hazy film with an adhesion promoting pretreatment on both sides

General Product Info: The pretreatment enables numerous solvent and UV inks and lacquers to be coated with excellent adhesion. The film is tear resistant, has excellent handling characteristics and also good dimensional stability when exposed to variations in temperature and humidity.

Typical Applications: This film was primarily developed for use in the Reprographics industry.

Approvals: UL Recognition - Product has been registered with Underwriters Laboratories

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Break, MD 193 MPa28000 psi50% strain rate; ASTM D882A
Film Tensile Strength at Break, TD 255 MPa37000 psi50% Strain rate; ASTM D882A
 
Thermal PropertiesMetricEnglishComments
Melting Point 255 - 260 °C491 - 500 °FASTM E794-85
Shrinkage, MD 2.5 %
@Temperature 190 °C,
Time 300 sec
2.5 %
@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Shrinkage, TD 0.50 %
@Temperature 190 °C,
Time 300 sec
0.50 %
@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
 
Optical PropertiesMetricEnglishComments
Haze  <= 9.0 %
@Thickness 0.0361 mm
<= 9.0 %
@Thickness 0.00142 in
Gardner Hazemeter; ASTM D1003-77
 <= 13 %
@Thickness 0.0500 mm
<= 13 %
@Thickness 0.00197 in
Gardner Hazemeter; ASTM D1003-77
 <= 14 %
@Thickness 0.0752 mm
<= 14 %
@Thickness 0.00296 in
Gardner Hazemeter; ASTM D1003-77
 <= 23 %
@Thickness 0.100 mm
<= 23 %
@Thickness 0.00394 in
Gardner Hazemeter; ASTM D1003-77
 <= 26 %
@Thickness 0.125 mm
<= 26 %
@Thickness 0.00493 in
Gardner Hazemeter; ASTM D1003-77

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Teijin Films Melinex® 544 Polyester Film, 380 Gauge
DuPont Teijin Films Melinex® 581 Polyester Film
DuPont Teijin Films Melinex® 565 Polyester Film
DuPont Teijin Films Melinex® 561 Polyester Film
DuPont Teijin Films Melinex® 583 Polyester Film, 300 Gauge

PDTZ9154 / 139509

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.