MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Socomore Aeroglaze® Z306 Absorptive Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Aeroglaze® Z306 absorptive polyurethane coating is primarily for applications to substrates used in space operations. These operations include those where coatings must exhibit low outgassing characteristics while providing high thermal absorptivity properties.

In addition, the mechanical properties required for rigorous durations in space are an integral part of the Aeroglaze Z306 absorptive polyurethane make-up. Aeroglaze Z306 absorptive polyurethane shows excellent performance on rigid or flexible substrates.

Socomore acquired the Aeroglaze® and Chemglaze® product lines from Lord in September 2016.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.950 g/cc0.0343 lb/in³ASTM D1475-85
Solids Content 23 %23 %by volume
 27 %27 %by weight
Volatile Organic Compounds (VOC) Content 692 g/l692 g/lASTM D3960-89
Brookfield Viscosity 60 cP
@Temperature 25.0 °C
60 cP
@Temperature 77.0 °F
ASTM D2196-86; LVT
Outgassing - Total Mass Loss 1.0 %1.0 %ASTM E595-77
 
Thermal PropertiesMetricEnglishComments
Flash Point 19.0 °C66.2 °FSetaflash, Closed Cup; ASTM D3278-82
 
Optical PropertiesMetricEnglishComments
Gloss <= 10 %<= 10 %85°
Emissivity (0-1) 0.900.90ASTM E408-71
 
Processing PropertiesMetricEnglishComments
Cure Time  720 min
@Temperature 25.0 °C
12.0 hour
@Temperature 77.0 °F
Permit Handling
 2160 - 2880 min
@Temperature 25.0 °C
36.0 - 48.0 hour
@Temperature 77.0 °F
Permit Normal Usage
Tack-Free Time 120 - 180 min
@Temperature 25.0 °C
2.00 - 3.00 hour
@Temperature 77.0 °F
50% RH
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
AppearanceFlat Black
Solar Absorption>0.95Gier-Dunkle Integrating Sphere
Theoretical Coverage (ft²/gallon/mil)368

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mateck Sapphire (Al2O3)
Titanium Ti-6Al-4V (Grade 5), Annealed Bar
Titanium Ti-6Al-4V (Grade 5), STA Bar
Mateck Sapphire Aluminium oxide Substrate, Al2O3
MarkeTech Sapphire (Aluminum Oxide - Al2O3) Single Crystal

PLORD129 / 86137

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.