MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Toyobo PELPRENE™ S2002FB Polyester TPE, Flame Resistant
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester TPE; Polyester, TP; Polyester Thermoplastic Elastomer

Material Notes: Features: Polyester TPE, Flame Resistant

Information provided by Toyobo.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.33 g/cc0.0480 lb/in³ASTM D792
Moisture Absorption at Equilibrium 0.38 %0.38 %23°C, 65% RH
Linear Mold Shrinkage 0.013 cm/cm
@Thickness 2.00 mm
0.013 in/in
@Thickness 0.0787 in
Melt Index of Compound 12 g/10 min
@Temperature 230 °C
12 g/10 min
@Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9898JIS K6301
Hardness, Shore D 5757ASTM D2240
Tensile Strength at Break 26.9 MPa3900 psiASTM D638
Elongation at Break 560 %560 %ASTM D638
50% Modulus 16.6 MPa
@Strain 50 %
16.6 MPa
@Strain 50 %
ASTM D638
Flexural Modulus 0.230 GPa33.4 ksiASTM D790
Compressive Modulus 0.0158 GPa2.29 ksi10%; ASTM D695
Resilience 6060JIS K6301
Izod Impact, Notched NBNBASTM D256
Tear Strength 160 kN/m913 pliASTM D624
Taber Abrasion, mg/1000 Cycles 1212ASTM D1044
Compression Set 65 %65 %JIS K6301
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 4.00e+13 ohm-cm4.00e+13 ohm-cmASTM D257
Dielectric Strength 25.0 kV/mm635 kV/inJIS K2111
 
Thermal PropertiesMetricEnglishComments
CTE, linear 130 µm/m-°C
@Temperature 20.0 °C
72.2 µin/in-°F
@Temperature 68.0 °F
TMA
Melting Point 210 °C410 °FBy DSC
Maximum Service Temperature, Air 110 °C230 °FHeat deflection temperature, load unknown; ASTM D648
Vicat Softening Point 185 °C365 °FASTM D1525
Brittleness Temperature <= -65.0 °C<= -85.0 °FJIS K6301
Flammability, UL94 V-2V-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Arnitel® UM551-V TPC-ES FR, Flame Retardant
Celanese Hytrel® G3548 NC010 TPC-ET
Envalior Arnitel® CM600-V TPC-ES FR, Extrusion, Flame Retardant
Toyobo Pelprene™ P-30B Polyester TPE
Toyobo PELPRENE™ P50DFR Polyester TPE, Flame Resistant

PTOY682 / 70842

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.