MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kraton® G1652 E (SEBS) Linear Block Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Description: Kraton G1652 E polymer is a clear, linear triblock copolymer based on styrene and ethylene/butylene, S-E/B-S, with bound styrene of 30% mass. It is supplied from Europe in the physical form shown:
Kraton G1652 EU - supplied as undusted fluffy crumb
Kraton G1652 ES - supplied as fluffy crumb dusted with amorphous silica

Region: Asia Pacific, Europe, Japan, North America, and South America

Uses: Kraton G1652 E is used as a modifier of bitumen or thermoplastics and in compound formulations. It is also suitable as an ingredient in formulating compounds for footwear applications and may be used in formulating adhesives, sealants and coatings.

Applications: Adhesives, Sealant and Coatings; Bitumen Modification; Compounding and Personal Hygiene; Impact Modification; Medical; Packaging and Polymod; and Personal Care

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.910 g/cc0.910 g/ccISO 2781
Volatiles <= 0.60 %<= 0.60 %KM 04
Brookfield Viscosity 400 - 530 cP
@Temperature 25.0 °C
400 - 530 cP
@Temperature 77.0 °F
25% Toluene solution
Melt Flow 6.0 g/10 min
@Load 5.00 kg,
Temperature 230 °C
6.0 g/10 min
@Load 11.0 lb,
Temperature 446 °F
ISO 1133
Ash 0.70 - 1.1 %0.70 - 1.1 %ISO 247
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 696910 seconds.; ASTM D 2240
Tensile Strength, Ultimate 31.03 MPa4501 psiASTM D412
Elongation at Break 500 %500 %ASTM D412
300% Modulus 4.83 MPa
@Strain 300 %
701 psi
@Strain 300 %
ASTM D412
 
Descriptive Properties
ContentAntioxidant>0.03%, KM 08
 Polystyrene28.2-30%, KM 03, polystyrene content measured on finished product after hydrogenation
 Total Extractables<1.0%, KM 05

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kraton® G1650 E (SEBS) Linear Block Copolymer
Kraton® FG1924 G (SEBS) Linear Block Copolymer
Kraton® G1654 E (SEBS) Linear Block Copolymer
Kraton® G1657 M (SEBS) Linear Block Copolymer
Kraton® G7723X

PKRA0250 / 49085

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.