MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Graft Polymer GRAFTALLOY™ LD-SAN 01000 Low Density Polyethylene – Styrene-Acrylonitrile
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: GRAFTALLOY™ LD-SAN 01000 is a high performance polymer alloy, consisting of LDPE, with chemically bound SAN. Its main characteristics are good compatibility with polyolefins, ABS, PLA, PC blends. Supplied as: Granulate. Applications:
  • Improve tribological properties
  • Improve Melt Flow Index of blends
  • mproves mechanical characteristics.
Processing: GRAFTALEN™ LD-SAN 01000 can be processed with all usual processing technologies (Injection molding, extrusion, blow molding, thermoforming...). Optimal processing temperatures are between 180°C and 200°C.

Information provided by Graft Polymer LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 35 g/10 min
@Load 2.16 kg,
Temperature 190 °C
35 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield >= 10.0 MPa>= 1450 psiInjection Molded. 10 mm/min; ISO 527-2
Elongation at Break 10 %10 %Injection molded. 10mm/min.; ISO 527-2
 
Thermal PropertiesMetricEnglishComments
Melting Point 100 °C212 °FDSC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Graft Polymer GRAFTABOND™ UH-SAN 00055 PDIM Ultra High Molecular Weight Polyethylene, grafted with Styrene Acrylonitrile
Graft Polymer GRAFTABOND™ SAN-MAH 01530 C Styrene Acrylonitrile Copolymer Grafted with Maleic Anhydride

PGRAFT942 / 232373

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.