MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical XR404 ABS, Heat Resistance
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded

Material Notes: Feature: Injection Molding, Heat Resistance

Application: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (Garnish etc)

CAS No. 25120-20-1, 9003-56-9 and 25747-74-7

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.05 g/cc1.05 g/ccASTM D792
Maximum Moisture Content 0.0100.010Injection Molding
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0040 - 0.0070 in/in
@Thickness 0.126 in
ASTM D955
Melt Flow 7.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
7.0 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 108108ASTM D785
Tensile Strength, Yield 48.1 MPa
@Thickness 3.20 mm
6970 psi
@Thickness 0.126 in
50 mm/min; ASTM D638
Elongation at Break 25 %
@Thickness 3.20 mm
25 %
@Thickness 0.126 in
50 mm/min; ASTM D638
Flexural Yield Strength 77.5 MPa
@Thickness 3.20 mm
11200 psi
@Thickness 0.126 in
15 mm/min; ASTM D790
Flexural Modulus 2.55 GPa
@Thickness 3.20 mm
370 ksi
@Thickness 0.126 in
15 mm/min; ASTM D790
Izod Impact, Notched  1.96 J/cm
@Thickness 6.40 mm,
Temperature 23.0 °C
3.67 ft-lb/in
@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
 2.16 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
4.04 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched  0.588 J/cm
@Thickness 6.40 mm,
Temperature -30.0 °C
1.10 ft-lb/in
@Thickness 0.252 in,
Temperature -22.0 °F
ASTM D256
 0.686 J/cm
@Thickness 3.20 mm,
Temperature -30.0 °C
1.29 ft-lb/in
@Thickness 0.126 in,
Temperature -22.0 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmASTM D257
Dielectric Strength 33.0 kV/mm
@Thickness 1.00 mm
838 kV/in
@Thickness 0.0394 in
ASTM D149
Arc Resistance 60 - 120 sec60 - 120 secASTM D495
Comparative Tracking Index >= 600 V>= 600 VSolution A; IEC 60112
Hot Wire Ignition, HWI  7.0 - 15 sec
@Thickness >=1.50 mm
7.0 - 15 sec
@Thickness >=0.0591 in
 15 - 30 sec
@Thickness >=3.00 mm
15 - 30 sec
@Thickness >=0.118 in
High Amp Arc Ignition, HAI  60 - 120 arcs
@Thickness 1.50 mm
60 - 120 arcs
@Thickness 0.0591 in
 >= 120 arcs
@Thickness 3.00 mm
>= 120 arcs
@Thickness 0.118 in
High Voltage Arc-Tracking Rate, HVTR 25.4 - 50.0 mm/min1.00 - 1.97 in/min
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 108 °C
@Thickness 6.40 mm
226 °F
@Thickness 0.252 in
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
@Thickness 6.40 mm
212 °F
@Thickness 0.252 in
Unannealed; ASTM D648
Vicat Softening Point 108 °C
@Load 5.00 kg
226 °F
@Load 11.0 lb
50°C/h; ASTM D1525
UL RTI, Electrical  60.0 °C
@Thickness >=1.50 mm
140 °F
@Thickness >=0.0591 in
UL 746B
 60.0 °C
@Thickness >=3.00 mm
140 °F
@Thickness >=0.118 in
UL 746B
UL RTI, Mechanical with Impact  60.0 °C
@Thickness >=1.50 mm
140 °F
@Thickness >=0.0591 in
UL 746B
 60.0 °C
@Thickness >=3.00 mm
140 °F
@Thickness >=0.118 in
UL 746B
UL RTI, Mechanical without Impact  60.0 °C
@Thickness >=1.50 mm
140 °F
@Thickness >=0.0591 in
UL 746B
 60.0 °C
@Thickness >=3.00 mm
140 °F
@Thickness >=0.118 in
UL 746B
Flammability, UL94  HB
@Thickness >=1.50 mm
HB
@Thickness >=0.0591 in
 HB
@Thickness >=3.00 mm
HB
@Thickness >=0.118 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 180 - 210 °C356 - 410 °FInjection Molding
Middle Barrel Temperature 210 - 230 °C410 - 446 °FInjection Molding
Front Barrel Temperature 230 - 240 °C446 - 464 °FInjection Molding
Nozzle Temperature 230 - 240 °C446 - 464 °FInjection Molding
Melt Temperature 220 - 240 °C428 - 464 °FInjection Molding
Mold Temperature 40.0 - 60.0 °C104 - 140 °FInjection Molding
Drying Temperature 80.0 - 90.0 °C176 - 194 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
Back Pressure 29.4 - 58.8 MPa4260 - 8530 psiInjection Molding
Screw Speed 50 - 100 rpm50 - 100 rpmInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical XR401 ABS, Heat Resistance
Lotte Advanced Materials Starex® SR-0320 K ABS, Unreinforced Heat Resistant
LG Chemical HP PMMA
LG Chemical XR401B ABS, High Flow, Heat Resistance
LG Chemical XR-401A ABS Resin

PLAY061 / 148069

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.