MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

LyondellBasell Purell PE 3040D Low Density Polyethylene (LDPE)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Blow Molding Grade

Material Notes: Purell PE 3040D is a low density polyethylene with high rigidity and good chemical resistance. It is delivered in pellet form. The grade is used for small blow molding including packaging of pharmaceuticals in blow fill seal technology and injection molding for medical devices, closures and seals. Applications: Blow-Fill-Seal Applications, Bottles and Vials, Healthcare Applications, Medical Devices, Medical Film

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density >= 0.500 g/cc>= 0.0181 lb/in³ISO 60
Density 0.928 g/cc0.0335 lb/in³ISO 1183-1
Melt Flow 0.25 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.25 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5151ISO 868
Tensile Strength, Yield 13.0 MPa1890 psiISO 527-1,-2
Tensile Modulus 0.300 GPa43.5 ksiISO 527-1,-2
 
Thermal PropertiesMetricEnglishComments
Melting Point 115 °C239 °FDSC; ISO 3146
Vicat Softening Point 102 °C216 °FA50N; ISO 306
 
Descriptive Properties
Processing MethodBlow, Fill, & Seal, Blown Film, Extrusion Blow Molding, Injection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Lupolen 3010D Low Density Polyethylene (LDPE), Blow Molding Grade
LyondellBasell Lucalen A2910M Low Density Polyethylene
LyondellBasell Hostalen GX 5058 High Density Polyethylene (HDPE), Pipe Grade
LyondellBasell Purell PE 3420F Low Density Polyethylene (LDPE)
Silon Taborex TA 1108 HD Chemically-Crosslinkable HDPE Compound

PEQT8635 / 220269

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.