MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Bayshore Vinyl Compounds BVC 1100-65 Clear PVC Compound
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Flexible Grade

Material Notes: BVC 1100-65 is a clear flexible PVC compound produced with FDA sanctioned ingredients. It is recommended for use in applications for the medical, food and beverage industries. This material offers excellent processing, stability and clarity for tubing, profile extrusions and some molding applications.

Information Provided by Bayshore Vinyl Compounds Inc., a Mexichem Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.18 g/cc1.18 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 62 - 68
@Time 10.0 sec
62 - 68
@Time 0.00278 hour
ASTM D2240
Tensile Strength at Break 15.62 MPa2266 psiASTM D638
Elongation at Break 466 %466 %ASTM D638
100% Modulus 5.47 MPa
@Strain 100 %
794 psi
@Strain 100 %
ASTM D638
Tear Strength 47.0 kN/m268 pliASTM D1004
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -44.0 °C-47.2 °FImpact Brittleness; ASTM D746
Clash Berg Stiffness Temperature -59.0 °C-74.2 °F135K; ASTM D1043
 -41.0 °C-41.8 °F35K; ASTM D1043
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %clear; thickness not quantified
 
Descriptive Properties
Activated Carbon@90°C, % Wt LossASTM D1203
Weight Loss (%), ASTM D12390.9Soapy H2O Extraction @ 50°C
 21.1Oil Extraction
 36Hexane Extraction

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Colorite Polymers 6588 Non-Phthalate 88 Series Vinyl Compound
Colorite Polymers Self Frosting™ 6511SF Vinyl Compound
DuPont Mobility and Materials Kalrez® 6221 FFKM Perfluoroelastomer
ExxonMobil Vyram™ 9201-65 Thermoplastic Elastomer
Geon® Performance Solutions Vinyl Flexible XV3796 Polyvinyl Chloride, Flexible

PBAYS002 / 93274

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.