MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Clyrell RC 215M Polypropylene
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: The specialty polypropylene Clyrell product portfolio includes random and impact copolymers based on Ziegler-Natta catalysts. Clyrell RC215M is a high flow and highly modified polypropylene random copolymer. It contains anti-blocking and slip additives. Clyrell RC215M is typically used for manufacturing of un-oriented films. Typical applications reported by customers are lamination, textile and packaging of foodstuffs. Customers have been reporting that films produced using Clyrell RC215M offer a good balance of properties such as high clarity, brightness, stiffness and medium seal initiation temperature (SIT). Applications: Food Packaging Film, Textile Packaging Film.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 22.0 MPa3190 psiASTM D882
Film Elongation at Break, MD 750 %750 %ASTM D 882
Coefficient of Friction 0.500.50ASTM D 1894
Film Tensile Strength at Break, MD 35.0 MPa5080 psiASTM D882
1% Secant Modulus, MD 660 MPa95700 psiASTM D 882
 
Optical PropertiesMetricEnglishComments
Haze <= 1.0 %
@Thickness 0.0500 mm
<= 1.0 %
@Thickness 0.00197 in
ASTM D1003
Gloss 90 %
@Thickness 0.0500 mm
90 %
@Thickness 0.00197 in
ASTM D 2457
 
Descriptive Properties
Processing MethodCast Film

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Apec® RW1697 Polycarbonate
Overview of materials for Nylon 6, 30% Glass Fiber Filled
Röhm PLEXIGLAS® XT Clear 0A070 UV transmitting PMMA
Borealis Bormed™ RB801CF Polypropylene Random Copolymer
LyondellBasell Moplen RP310M Polypropylene Copolymer

PEQT7085 / 218723

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.