MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® 8333G HI 33% Glass Filled PA6 (Conditioned)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: Ultramid 8333G HI is a 14% glass reinforced, impact modified PA6 injection molding compound developed for applications requiring improved dry as molded toughness in combination with a balance of strength, stiffness and excellent moldability/surface aesthetics. It is also available in heat stabilized (Ultramid 8331G HI HS) and/or pigmented versions.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.34 g/cc0.0484 lb/in³dry; ISO 1183
Melt Density 1.16 g/cc
@Temperature >=220 °C
0.0419 lb/in³
@Temperature >=428 °F
ISO 1183
Water Absorption 0.90 %0.90 %24 hour; ISO Test
 5.5 %5.5 %beginning dry; ISO 62
Moisture Absorption at Equilibrium 1.5 %1.5 %beginning dry (23°C/50% R.H.); ISO 62
Linear Mold Shrinkage 0.0030 cm/cm0.0030 in/inASTM Data; MD
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 90.0 MPa13100 psi0.2 in/min; ASTM Test
Tensile Strength, Ultimate 90.0 MPa13100 psi5mm/min; ISO 527
Elongation at Break 6.0 %6.0 %5mm/min; ISO 527
 6.0 %6.0 %0.2 in/min; ASTM Test
Tensile Modulus 4.61 GPa669 ksi1mm/min; ISO 527
Flexural Strength 120 MPa17400 psiISO Data
 124 MPa18000 psiASTM Test
 90.0 MPa
@Temperature 120 °C
13100 psi
@Temperature 248 °F
ASTM Test
 100 MPa
@Temperature 93.0 °C
14500 psi
@Temperature 199 °F
ASTM Test
 110 MPa
@Temperature 65.0 °C
16000 psi
@Temperature 149 °F
ASTM Test
 297 MPa
@Temperature -40.0 °C
43100 psi
@Temperature -40.0 °F
ASTM Test
Flexural Modulus 4.83 GPa701 ksiASTM Test
 5.03 GPa730 ksiISO Data
 2.97 GPa
@Temperature 120 °C
431 ksi
@Temperature 248 °F
ASTM Test
 3.25 GPa
@Temperature 93.0 °C
471 ksi
@Temperature 199 °F
ASTM Test
 3.29 GPa
@Temperature 65.0 °C
477 ksi
@Temperature 149 °F
ASTM Test
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.958 J/g-°C0.4680 BTU/lb-°FMelt
Thermal Conductivity 0.200 W/m-K1.39 BTU-in/hr-ft²-°FMelt
Melting Point 220 °C428 °F10 K/min
 220 °C428 °FASTM Test
 
Processing PropertiesMetricEnglishComments
Melt Temperature 275 °C527 °FInjection molding
Mold Temperature 95.0 °C203 °FInjection molding
 
Descriptive Properties
ColorNatural
Commercial StatusActive America
FormPellets
Impact ModifiedYes
Primary Processing TechniqueInjection Molding
ProcessingInjection Molding
UL.UL-CYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® 8333G HI 33% Glass Filled PA6 (Dry)
BASF Capron® 8333G HI Impact Modified, 33% Glass-Filled Nylon 6 (Dry)
BASF Ultramid® 8333G HI HS BK 106 33% Glass Filled PA6 (Conditioned)
BASF Ultramid® 8333G HI HS BK-102 33% Glass Filled PA6 (Conditioned)
BASF Ultramid® 8333G HI HS BK 106 33% Glass Filled PA6 (Dry)

PBASF9202 / 84966

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.