MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Envalior Stanyl® TW271B6 (PA46+PTFE)-CF30, Dry, 30% Carbon Fiber, Heat Stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 46 (PA46)

Material Notes: 30% Carbon Reinforced, Heat Stabilized, Wear and Friction Modified

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.32 g/cc0.0477 lb/in³ISO 1183
Moisture Absorption 2.40 %2.40 %Humidity; Sim. ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cm0.0030 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0070 cm/cm0.0070 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 260 MPa37700 psiISO 527-1/-2
 95.0 MPa
@Temperature 200 °C
13800 psi
@Temperature 392 °F
ISO 527-1/-2
 105 MPa
@Temperature 180 °C
15200 psi
@Temperature 356 °F
ISO 527-1/-2
 115 MPa
@Temperature 160 °C
16700 psi
@Temperature 320 °F
ISO 527-1/-2
 140 MPa
@Temperature 120 °C
20300 psi
@Temperature 248 °F
ISO 527-1/-2
Elongation at Break 1.7 %1.7 %ISO 527-1/-2
 3.1 %
@Temperature 120 °C
3.1 %
@Temperature 248 °F
ISO 527-1/-2
 3.1 %
@Temperature 160 °C
3.1 %
@Temperature 320 °F
ISO 527-1/-2
 3.1 %
@Temperature 180 °C
3.1 %
@Temperature 356 °F
ISO 527-1/-2
 3.1 %
@Temperature 200 °C
3.1 %
@Temperature 392 °F
ISO 527-1/-2
Tensile Modulus 24.0 GPa3480 ksiISO 527-1/-2
 11.0 GPa
@Temperature 200 °C
1600 ksi
@Temperature 392 °F
ISO 527-1/-2
 11.5 GPa
@Temperature 180 °C
1670 ksi
@Temperature 356 °F
ISO 527-1/-2
 12.0 GPa
@Temperature 160 °C
1740 ksi
@Temperature 320 °F
ISO 527-1/-2
 13.5 GPa
@Temperature 120 °C
1960 ksi
@Temperature 248 °F
ISO 527-1/-2
Charpy Impact Unnotched  5.00 J/cm²
@Temperature 23.0 °C
23.8 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
 5.00 J/cm²
@Temperature -30.0 °C
23.8 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched  0.700 J/cm²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 0.700 J/cm²
@Temperature -30.0 °C
3.33 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 25.0 µm/m-°C13.9 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 35.0 µm/m-°C19.4 µin/in-°FISO 11359-1/-2
Melting Point 295 °C563 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 290 °C554 °FISO 72-1/-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Stanyl® TW271B6 (PA46+PTFE)-CF30
Ensinger Tecapeek® XP-119G Compression Molded PEEK Compound, 10% Carbon Fiber with 5% Graphite
Envalior Stanyl® TW271B6 (PA46+PTFE)-CF30, Conditioned, 30% Carbon Fiber, Heat Stabilized
Ensinger Tecapeek® XP-113 Compression Molded PEEK Compound, 10% PTFE, 15% Graphite, and 3% Carbon Fiber
Akro-Plastic Akrotek® PEEK CF 30 black (5049) PEEK, Dry, 30% Carbon Filled

PDSM8250 / 184951

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.