MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Rubatex G231 Neoprene Rubber Foam Sheet  (discontinued **)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Information provided by Rubatex.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.160 - 0.320 g/cc0.00579 - 0.0116 lb/in³ASTM D 1056
Water Absorption <= 5.0 %<= 5.0 %0.1 lb/ft² per ASTM D 1667; ASTM D 1056
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore OO 25 - 4025 - 40
Tensile Strength, Ultimate >= 0.517 MPa>= 75.0 psiASTM D 412
Elongation at Break >= 450 %>= 450 %ASTM D 412
Resilience 50 - 6550 - 65% Bashore; 1/2* thickness @ 72F
Compression Set <= 25 %<= 25 %Based on compressed height; ASTM D 1056
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.0432 W/m-K0.300 BTU-in/hr-ft²-°FK factor; ASTM C 177
Maximum Service Temperature, Air 93.3 °C200 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °FCold Crack; ASTM D 1056
Shrinkage <= 10 %
@Temperature 70.0 °C,
Time 605000 sec
<= 10 %
@Temperature 158 °F,
Time 168 hour
Linear; ASTM C 534
 
Descriptive Properties
ASTM D 1056-002C1
ASTM D 1056-67SCE41
ColorBlack
Compression Deflection (25%)2-5 psiASTM D 1056
Compression Deflection Heat AgingMax Change +/-30%ASTM D 1056
Expected Yield Thickness (In.).50After 2 level cuts
Flammability RatingPASSES FMVSS302
Fluid Immersion <150 Wt%ASTM D 1056; Based on ASTM Ref. Fuel B.
Mil R 6130 TYPE 2/ASTM D6576-00 GradeAorB/Soft
Ozone Resistance Rating0ASTM D 1171 (72 HOURS 50PPHM)
Sheet Size (In.)40X120Other sizes may be available
UL 50/508Yes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Rubatex R411 Neoprene Rubber Foam Sheet
Denka Neoprene 671A Polychloroprene
Rubatex R4261 Flame Retardant Neoprene/EPDM/SBR Rubber Foam Sheet
Rubatex R426 Neoprene/EPDM/SBR Rubber Foam Sheet
Rubatex R421 Neoprene/EPDM/SBR Rubber Foam Sheet

PRUBAT30 / 66493

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.