MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow AFFINITY™ GA 1950 Polyolefin Plastomer (POP)
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: AFFINITY™ GA 1950 Polyolefin Plastomer (POP) is produced via INSITE™ Technology from Dow Plastics. This product can be used in applications such as polymer modification (i.e. flow enhancement and property enhancement), masterbatch / additive carrier, and hot melt adhesives.

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.874 g/cc0.0316 lb/in³ASTM D792
Brookfield Viscosity 17000 cP
@Temperature 177 °C
17000 cP
@Temperature 350 °F
ASTM D1084
Collected Volatile Condensable Material <= 0.15 %<= 0.15 %Modified for polyolefins. Change in temperature used to 100°C ± 3 and the amount of sample to 20 grams.; ASTM D3030
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 1.76 MPa255 psiASTM D638
Elongation at Break 185 %185 %ASTM D638
 
Thermal PropertiesMetricEnglishComments
Melting Point 70.0 °C158 °FDow Method
Glass Transition Temp, Tg -57.0 °C-70.6 °FDow Method
 
Optical PropertiesMetricEnglishComments
Gardner Color Number 1.01.0ASTM D3417

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow AFFINITY™ GA 1900 Polyolefin Plastomer (POP)
Dow AFFINITY™ EG 8185 Polyolefin Plastomer (POP)
Dow AFFINITY™ EG 8200G Ethylene alpha-olefin copolymer
Dow AFFINITY™ EG 8150G Ethylene alpha-olefin copolymer
Dow AFFINITY™ PT 1450G1 Ethylene alpha-olefin resin

PDOW1169 / 30387

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.