MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® A3ZG6 BK 20591 30% Glass Filled PA66 (Conditioned)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Description: Impact-modified, 35% glass-fiber reinforced injection-molding grade.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.33 g/cc0.0480 lb/in³ISO 1183
Moisture Absorption at Equilibrium 1.3 - 1.7 %1.3 - 1.7 %23°C; 50% RH; ISO 62
Water Absorption at Saturation 4.7 - 5.3 %4.7 - 5.3 %ISO 62
Viscosity Measurement 160160ISO 307
Linear Mold Shrinkage 0.0055 cm/cm0.0055 in/inrestricted
Melt Flow 19.95 g/10 min
@Load 5.00 kg,
Temperature 275 °C
19.95 g/10 min
@Load 11.0 lb,
Temperature 527 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 100 MPa14500 psi50 mm/min; ISO 527-1/-2
Elongation at Yield 6.0 %6.0 %50 mm/min; ISO 527-1/-2
Modulus of Elasticity 6.00 GPa870 ksiISO 527-1/-2
Flexural Strength 150 MPa21800 psiat max force; ISO 178
Flexural Modulus 4.90 GPa711 ksiISO 178
Izod Impact, Notched (ISO)  18.0 kJ/m²
@Temperature -30.0 °C
8.57 ft-lb/in²
@Temperature -22.0 °F
ISO 180/A
 20.0 kJ/m²
@Temperature 23.0 °C
9.52 ft-lb/in²
@Temperature 73.4 °F
ISO 180/A
Charpy Impact Unnotched 9.50 J/cm²
@Temperature 23.0 °C
45.2 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 2.60 J/cm²
@Temperature 23.0 °C
12.4 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
Tensile Creep Modulus, 1000 hours 3000 MPa
@Strain <=0.5 %
435000 psi
@Strain <=0.5 %
ISO 899-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+10 ohm-cm1.00e+10 ohm-cmIEC 60093
Surface Resistance 1.00e+10 ohm1.00e+10 ohmIEC 60093
Dielectric Constant 5.5
@Frequency 1e+6 Hz
5.5
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.16
@Frequency 1e+6 Hz
0.16
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 550 V550 VTest solution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.70 J/g-°C0.406 BTU/lb-°F
Thermal Conductivity 0.350 W/m-K2.43 BTU-in/hr-ft²-°FDIN 52612
Melting Point 260 °C500 °FDIN 53765
Maximum Service Temperature, Air 220 °C428 °F
Decomposition Temperature >= 310 °C>= 590 °F
Ignition Temperature >= 400 °C>= 752 °FASTM D129
 
Processing PropertiesMetricEnglishComments
Processing Temperature 80.0 °C176 °FHopper Throat
Zone 1 290 °C554 °FFeed Zone
Zone 2 290 °C554 °FCompression
Zone 3 290 °C554 °FMetering-zone
Zone 4 290 °C554 °FNozzle
Melt Temperature 280 - 300 °C536 - 572 °FInjection-molding/Extrusion
 290 °C554 °FOptimal
Mold Temperature 80.0 °C176 °FOptimal
 80.0 - 90.0 °C176 - 194 °FInjection-molding
Drying Temperature 80.0 °C176 °F
Dry Time 4 hour4 hour
Moisture Content 0.030 - 0.060 %0.030 - 0.060 %Optimal
 <= 0.15 %<= 0.15 %
 
Descriptive Properties
ColorBK 20591
Commercial StatusEurope
Peripheral Screw Speed< 0.3 m/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 66, 30% Glass Fiber Filled
BASF Ultramid® A3HG6 HR BK 23591 30% Glass Filled PA66 (Conditioned)
BASF Ultramid® A3EG6 30% Glass Filled PA66 (Conditioned)
BASF Capron® GR630 HS 30% Glass-Filled Nylon 66 (Dry)
BASF Capron® GR630 HS 30% Glass-Filled Nylon 66 (Conditioned)

PBASG0249 / 131882

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.