MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ChevronTexaco SAE 30 Transmission and Drive Train TO-4 Oil
Categories: Fluid; Lubricant

Material Notes: Texaco Transmission and Drive Train TO-4 Oils deliver value through:
  • Longer equipment life — Special additives protect metal surfaces against scuffing and wear even under severe operating conditions of high temperature and high load.
  • Smoother operation — Excellent frictional control prevents clutch slippage and assures quiet and efficient action of transmission and brakes while reducing wear.
  • Reduced downtime — Good compatibility with seals, O rings, and packing materials maintains their good condition and keeps leakage at a minimum.
  • Longer oil life — Outstanding ability of the base stock to withstand oxidation at high operating temperatures results in increased service life for the oil.
  • More reliable operation — Formulation keeps metal parts clean and free of varnish and sludge deposits that could result in premature breakdown.
  • Minimizing weather and storage concerns — Protects against rust and corrosion of highly finished precision parts when operating in humid conditions and during seasonal shutdown periods.

Texaco Transmission and Drive Train TO-4 Oils are high performance lubricants designed for use in transmissions, final drives, and hydraulic systems requiring a fluid meeting Caterpillar TO-4 or Allison C4 requirements.

They are manufactured using highly refined base oils, detergents, dispersants, oxidation and corrosion inhibitors, antiwear and extreme pressure agents, and a foam suppressant.

Texaco Transmission and Drive Train TO-4 Oils are designed for both newly developed and older model drive train components.

They offer excellent friction retention, wear control, seal compatibility, oxidation stability, and viscosity stability.

The frictional characteristics of the fluid are retained over the life of the lubricant.

Components are protected from wear, even in severe service and under high loads. They protect precision parts against wear under high load conditions by controlling the formation of corrosion, varnish, and sludge.

Texaco Transmission and Drive Train TO-4 Oils are compatible with new and traditional seal and clutch materials.

Texaco Transmission and Drive Train TO-4 Oils are recommended for use in Caterpillar transmissions, final drives, wet brakes, Allison Powershift transmissions, torque converters, and hydraulic systems requiring a fluid meeting Allison C4 or Caterpillar TO-4 or TO-2 requirements.

Under normal ambient temperatures, hydraulic systems will use the SAE 10W viscosity grade. SAE 10W and 30 are recommended for mobile hydraulic systems where operating requirements are severe.

Transmissions will use the SAE 30 viscosity grade. Texaco Transmission and Drive Train TO-4 Oils are also recommended for heavy duty off highway automatic transmissions requiring an SAE 10W, 30, 50, or 60 fluid.

Final drives will use the SAE 50 viscosity grade at normal temperatures and the SAE 60 at high ambient temperatures.

Texaco Transmission and Drive Train TO-4 Oils are not recommended for use in combined farm tractor hydraulic and transmission systems where low brake chatter is a requirement.

Texaco Transmission and Drive Train TO-4 Oils meet:

  • Service requirements of Caterpillar TO-4
  • Requirements of Allison C4 (SAE 10W, 30)

Do not use in high pressure systems in the vicinity of flames, sparks and hot surfaces. Use only in well ventilated areas. Keep container closed.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

CPS Number: 221954; MSDS Number: 8678

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
API Gravity 29.4 °29.4 °
Viscosity Measurement 100100Viscosity Index
Saybolt Viscosity at 100°F 431 SUS431 SUS
Saybolt Viscosity at 210°F 60 SUS60 SUS
Kinematic Viscosity at 40°C (104°F) 83 cSt83 cSt
Kinematic Viscosity at 100°C (212°F) 10 cSt10 cSt
 
Thermal PropertiesMetricEnglishComments
Pour Point -24.0 °C-11.2 °F
Flash Point 255 °C491 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LNP Lubricomp® DFL-4032 BK8-250 Polycarbonate, Glass Fiber Reinforcement, PTFE Lubricant
Kotec Carbotex KGN-20MRA Polycarbonate, Flame Retardant, 20% Glass Fiber Reinforced
Kotec Carbotex KGN-10MRA Polycarbonate, Flame Retardant, 10% Glass Fiber Reinforced
Henkel Loctite® 3301 Light Cure Acrylic Adhesive
Henkel Loctite® 3101 Acrylic Light Cure Adhesive

WTEXA210 / 77089

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.