MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chi Mei Kibisan® PN137H SAN Resin, General Purpose
Categories: Polymer; Thermoplastic; SAN Polymer; Styrene Acrylonitrile (SAN), Molded

Material Notes: Information provided by Calsak Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.06 g/cc1.06 g/ccASTM D792
Melt Flow 0.90 g/10 min
@Load 5.00 kg,
Temperature 200 °C
0.90 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 86
@Thickness 6.35 mm
86
@Thickness 0.250 in
ASTM D788
Tensile Strength, Yield 78.74 MPa
@Thickness 3.17 mm
11420 psi
@Thickness 0.125 in
6 mm/min; ASTM D638
Elongation at Yield 5.0 %
@Thickness 3.17 mm
5.0 %
@Thickness 0.125 in
6 mm/min; ASTM D638
Flexural Yield Strength 112.5 MPa
@Thickness 6.35 mm
16310 psi
@Thickness 0.250 in
2.8 mm/min; ASTM D790
Flexural Modulus 3.79 GPa
@Thickness 6.35 mm
550 ksi
@Thickness 0.250 in
2.8 mm/min; ASTM D790
Izod Impact, Notched  0.187 J/cm
@Thickness 6.35 mm,
Temperature 23.0 °C
0.350 ft-lb/in
@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D256
 0.224 J/cm
@Thickness 3.17 mm,
Temperature 23.0 °C
0.420 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi)  95.0 °C
@Thickness 6.35 mm
203 °F
@Thickness 0.250 in
unannealed, 120°C/hr; ASTM D648
 104 °C
@Thickness 6.35 mm
219 °F
@Thickness 0.250 in
annealed, 120°C/hr; ASTM D648
Vicat Softening Point 110 °C
@Thickness 3.17 mm
230 °F
@Thickness 0.125 in
50°C/hr; ASTM D1525
Flammability, UL94 HB
@Thickness 1.59 mm
HB
@Thickness 0.0625 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chi Mei Kibisan® PN-127H SAN
Chi Mei Kibisan® PN107 SAN Resin, General Purpose
Chi Mei Kibisan® PN-107 L125 SAN
Chi Mei Kibisan® PN-106 L150 SAN
Versalis KOSTIL PD C365 Styrene Acrylonitrile

PLBZ72 / 50541

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.