MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Solvay Chemicals CASO® FEED POWDER Calcium Chloride
Categories: Ceramic; Halide

Material Notes: Solvay is manufacturing and placing on the market dihydrate calcium chloride (CASO®FEED), feed material of mineral origin in conformity with European Directive 2002/32/EU and its amendments on undesirable substances in animal feed.

REACH Registration Number: 01-2119494219-28/ CAS number: 10035-04-8/ EINECS - N°: 233-140-8/ CE - N°: 017-013-00-2

Applications: CASO® Feed, calcium chloride, is classified as feed material for animal nutrition according to the European Regulation N° 68/2013 (RM 11.1.6). CASO® Feed is manufactured with consideration of HACCP principles as established in the Regulation (EC) N° 183/2005 and its successive amendments about Feed Hygiene

Information provided by Solvay

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.800 - 0.900 g/cc0.0289 - 0.0325 lb/in³
Molecular Weight 147.02 g/mol147.02 g/mol
 
Descriptive Properties
AppearancePowder
ColorWhite
Composition<0.1 mg/kgHg
 <0.1 mg/kgHg, Specifications
 <10 mg/kgPb, Specifications
 <15 mg/kgNaNO2, Specifications
 <150 mg/kgFluorides, Specifications
 <2 mg/kgCd, Specifications
 <2 mg/kgAs
 <2 mg/kgAs, Specifications
 <40 mg/kgFluorides
 >270 g/kgCa, Specifications
 >480 g/kgCl, Specifications
 >750 g/kgCaCl2, Specifications
 0.04 mg/kgCd
 1.1 g/kgCa(OH)2
 1.8 g/kgSO4
 10 mg/kgNaNO2
 2.1 mg/kgPb
 27 g/kgNaCl
 290 g/kgCa
 513 g/kgCl
 804 g/kgCaCl2
Granulometry100 percent<2.0 mm, statistical average
 100 percent<2.0 mm, typical value
 60 percent<0.5 mm, statistical average
 65 percent<1.0 mm, statistical average
 70 percent<0.5 mm, typical value
 85 percent<1.0 mm, typical value

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay Chemicals CASO® FOOD FLAKES Food additive E 509, Calcium Chloride
Solvay Chemicals CASO® Granular Anhydrous Calcium Chloride >94%
Solvay Chemicals CASO® TECHNICAL FLAKES LOW SULPHATES Calcium Chloride
Solvay Chemicals CASO® TECHNICAL FLAKES Calcium Chloride
Solvay Chemicals CASO® SIEVED FLAKES Calcium Chloride

WSOLV121 / 147770

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.