MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

P & P Technology Stainless Steel (Alloy 304) Knitted Cored Shielding Mesh
Categories: Metal; Ferrous Metal; Stainless Steel; T 300 Series Stainless Steel

Material Notes: Product has a diameter of 0.11mm.

Information provided by P & P Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Electrical PropertiesMetricEnglishComments
Shielding Effectiveness  40 dB
@Frequency 10000 Hz
40 dB
@Frequency 10000 Hz
H-Field
 44 dB
@Frequency 100000 Hz
44 dB
@Frequency 100000 Hz
H-Field
 58 dB
@Frequency 1e+6 Hz
58 dB
@Frequency 1e+6 Hz
H-Field
 60 dB
@Frequency 1e+10 Hz
60 dB
@Frequency 1e+10 Hz
P-Field
 76 dB
@Frequency 1e+9 Hz
76 dB
@Frequency 1e+9 Hz
P-Field
 94 dB
@Frequency 4.00e+8 Hz
94 dB
@Frequency 4.00e+8 Hz
P-Field
 100 dB
@Frequency 1e+8 Hz
100 dB
@Frequency 1e+8 Hz
E-Field
 120 dB
@Frequency 1e+7 Hz
120 dB
@Frequency 1e+7 Hz
E-Field
 125 dB
@Frequency 1e+6 Hz
125 dB
@Frequency 1e+6 Hz
E-Field

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Pyrotek Stainless Steel Mesh Core
416 Stainless Steel, annealed wire 6.4 mm diameter
416 Stainless Steel, annealed bar
304 Stainless Steel
Ashley Polymers Ashlene® PC/ABS Alloy 304

PPPTEC014 / 133478

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.