High Heat, Low Gloss, Medium Impact ABS resin for injection molded automotive interior trim applications. Application: - Chrysler-MSDB-300, MSDB-191
- Ford-WSB-M4D690-A
- GM-GMP.ABS.009
Automotive Specifications:- FORD WSS-M4D690-B1
- GM GMW15572P-ABS-T2
- VAG VW-TL-527
- VAG VW-TL-527 A
Data provided by Dow Chemical. This product line was spun off from Dow Chemical to Styron in 2010. |
Poly(Acrylonitrile Butadiene Styrene) |