MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Morgan Advanced Ceramics Nilcra® Zirconia TS Grade Mg-PSZ
Categories: Ceramic; Oxide; Zirconium Oxide

Material Notes: Description:
  • Magnesia-Partially Stabilised Zirconia (Mg-PSZ) with exceptional transformation toughening properties
  • Comprising 3.5 wt% MgO in ZrO2
  • Designed for applications requiring high thermal shock resistance
Prime Features:
  • Very high mechanical strength
  • Excellent wear and abrasion resistance
  • Excellent corrosion resistance
  • High impact resistance and toughness
  • Superior thermal shock resistance
  • Very low thermal conductivity
Typical Applications:
  • Excellent for combating wear and corrosion in applications requiring thermal shock resistance
  • Successfully used for a wide variety of tooling used in metal forming, such as, dies for hot copper and brass extrusion, guide rollers for welded tube production and for zinc coating steel sheet
Production Capabilities:
  • Sintered components
  • Precision ground components
  • Ceramic / Metal assemblies
  • Ceramic design assistance

Information provided by Morgan Advanced Materials

Key Words: Nilcra ®
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 5.74 g/cc
@Temperature 20.0 °C
0.207 lb/in³
@Temperature 68.0 °F
Grain Size 45 µm45 µm
Weibull Modulus >= 30
@Temperature 20.0 °C
>= 30
@Temperature 68.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 1020
@Temperature 20.0 °C
1020
@Temperature 68.0 °F
[kg/mm2], HV0.3
Tensile Strength 390 MPa
@Temperature 20.0 °C
56600 psi
@Temperature 68.0 °F
Modulus of Elasticity 205 GPa
@Temperature 20.0 °C
29700 ksi
@Temperature 68.0 °F
Flexural Strength  360 MPa
@Temperature 820 °C
52200 psi
@Temperature 1510 °F
4pt bend
 650 MPa
@Temperature 20.0 °C
94300 psi
@Temperature 68.0 °F
4pt bend
Compressive Strength  1750 MPa
@Temperature 20.0 °C
254000 psi
@Temperature 68.0 °F
 1800 MPa
@Temperature 20.0 °C
261000 psi
@Temperature 68.0 °F
Poissons Ratio 0.31
@Temperature 20.0 °C
0.31
@Temperature 68.0 °F
Fracture Toughness 14.0 - 16.0 MPa-m½
@Temperature 20.0 °C
12.7 - 14.6 ksi-in½
@Temperature 68.0 °F
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity  8000 ohm-cm
@Temperature 900 °C
8000 ohm-cm
@Temperature 1650 °F
 27000 ohm-cm
@Temperature 600 °C
27000 ohm-cm
@Temperature 1110 °F
 190000 ohm-cm
@Temperature 500 °C
190000 ohm-cm
@Temperature 932 °F
 >= 1.00e+11 ohm-cm
@Temperature 20.0 °C
>= 1.00e+11 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  9.70 µm/m-°C
@Temperature 25.0 - 800 °C
5.39 µin/in-°F
@Temperature 77.0 - 1470 °F
 9.90 µm/m-°C
@Temperature 25.0 - 400 °C
5.50 µin/in-°F
@Temperature 77.0 - 752 °F
Specific Heat Capacity 0.470 J/g-°C
@Temperature 20.0 °C
0.112 BTU/lb-°F
@Temperature 68.0 °F
Thermal Conductivity  2.32 W/m-K
@Temperature 800 °C
16.1 BTU-in/hr-ft²-°F
@Temperature 1470 °F
 2.47 W/m-K
@Temperature 400 °C
17.1 BTU-in/hr-ft²-°F
@Temperature 752 °F
 3.05 W/m-K
@Temperature 20.0 °C
21.2 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
 
Component Elements PropertiesMetricEnglishComments
MgO 3.5 %3.5 %in ZrO2
 
Descriptive Properties
Colorwhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Carpenter Advanced Ceramics TS Grade Zirconia
Morgan Advanced Ceramics Nilcra® Zirconia TS Technical Ceramic
CeramTec ZN 40 Zirconia, ZrO2-MgO
CoorsTek Yttria Partially Stabilized Zirconia, YTZP, Sintered
Ferro Zirmonite 1000, TZP

CMORF5080 / 200318

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.