MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ArcelorMittal Extragal® Z100 Double-sided pure zinc galvanized steel
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Applications: Because of their high corrosion protection capacity and surface quality, Extragal® coated products are recommended for numerous automotive applications, for both visible and non-visible parts. The Extragal® production process, involving a continuous single-step operation after rolling, makes it nearly always the most cost effective pre-coating solution for obtaining the corrosion resistance required in automotive sheet applications.

Technical characteristics:

Surface appearance: The crystal structure of Extragal® coatings is not visible to the naked eye. The high surface quality leads to a finished paint appearance meeting the severest requirements of the automotive industry for visible bodywork parts.

Hardness: Extragal® coatings are relatively ductile, with limited risk of damage in the drawing tools

Information provided by ArcelorMittal

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Coating Weight 50.0 - 65.0 g/m²31.3 - 40.6 lb/reamper side
 >= 100 g/m²>= 62.5 lb/reamdouble-sided

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ASTM A525 Galvanized Steel
ASTM A525M Galvanized Steel
ASTM A526 Galvanized Steel
ASTM A528 Galvanized Steel
ASTM A642 Galvanized Steel

NARCE080 / 159988

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.