MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro DESMODUR® 0363 + BAYTEC® XL 0328 + BAYTEC® 0354 + BAYTEC® 0340 92A Polyurethane, MDI PPG
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes:

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.01 g/cc1.01 g/ccat processing temp, BAYTEC® XL 0328
 1.037 g/cc1.037 g/ccat processing temp, BAYTEC® 0340
 1.038 g/cc1.038 g/ccat processing temp, BAYTEC® 0354
 1.09 g/cc1.09 g/ccat processing temp, DESMODUR® 0363
Viscosity 200 cP200 cPat processing temp, BAYTEC® 0340
 900 cP900 cPat processing temp, BAYTEC® XL 0328
 2000 cP2000 cPat processing temp, BAYTEC® 0354
 2750 cP2750 cPat processing temp, DESMODUR® 0363
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9292DIN 53505
Tensile Strength at Break 34.0 MPa4930 psiDIN 53504
Elongation at Break 450 %450 %DIN 53504
100% Modulus 9.00 MPa
@Strain 100 %
1310 psi
@Strain 100 %
DIN 53504
300% Modulus 17.5 MPa
@Strain 300 %
2540 psi
@Strain 300 %
DIN 53504
Resilience 4242[%]
Tear Strength 42.1 kN/m240 pliISO 34-1
Abrasion 7474[mm3]; ISO 4649
Compression Set 90 %
@Temperature 70.0 °C,
Time 86400 sec
90 %
@Temperature 158 °F,
Time 24.0 hour
ISO 815-1
 
Processing PropertiesMetricEnglishComments
Processing Temperature 25.0 °C77.0 °FDESMODUR® 0363
 25.0 °C77.0 °FBAYTEC® 0354
 25.0 °C77.0 °FBAYTEC® 0340
 30.0 °C86.0 °FBAYTEC® XL 0328
Mold Temperature 25.0 °C77.0 °F
 
Descriptive Properties
AppearanceliquidDESMODUR® 0363
 liquidBAYTEC® XL 0328
 liquidBAYTEC® 0354
 liquidBAYTEC® 0340
Content175.2Parts by weight of BAYTEC® 0363
 20Parts by weight of BAYTEC® XL 0328
 80Parts by weight of 0 BAYTEC® 354

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro DESMODUR® LU-D80 + MOCA Polyurethane, TDI-Ester
Covestro Desmodur® 30BV30 + (Baytec® 20BV29 + Baytec® XL9611 + Baytec® XL B) 88A Polyurethane, MDI Ester
Covestro Desmodur® 30BV30 + (Baytec® 20BV29 + Baytec® XL9611 + Baytec® XL B) 72A Polyurethane, MDI Ester
Covestro Desmodur® 30BV30 + (Baytec® 20BV29 + Baytec® XL9611 + Baytec® XL B) 62A Polyurethane, MDI Ester
Covestro Desmodur® 30BV30 + (Baytec® 20BV29 + Baytec® XL9611 + Baytec® XL B) 93A Polyurethane, MDI Ester

PCOVEST0325 / 202108

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.