MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Domo TECHNYL® B 218 Black 21 N PA66/6, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66

Material Notes: Description: Unreinforced copolyamide PA 66/6 , heat stabilized , medium viscosity, for injection molding.

Available in: Europe

Product Applications: TECHNYL® B 218 offers all of the primary properties of unreinforced polyamide 66 .In addition , it has improved resistance to high temperature , and can be used for components which will withstand long-term temperature stresses , such as: Automotive industry- diagnostic plugs, ashtray bodies and covers. Electrical industry- housings, connectors, terminal blocks . This product is available in natural, black and grey.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ISO 1183/A
Water Absorption 1.6 %
@Temperature 23.0 °C,
Time 86400 sec
1.6 %
@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Linear Mold Shrinkage 0.010 cm/cm0.010 in/inIsotropy
Linear Mold Shrinkage, Flow 0.014 cm/cm0.014 in/in
Linear Mold Shrinkage, Transverse 0.014 cm/cm0.014 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 75.0 MPa10900 psiISO 527 Type 1A
Tensile Strength, Yield 95.0 MPa13800 psiISO 527 type 1 A
Elongation at Break 30 %30 %ISO 527 Type 1A
Elongation at Yield 5.0 %5.0 %ISO 527 type 1 A
Tensile Modulus 3.00 GPa435 ksiISO 527 Type 1A
Flexural Strength 125 MPa18100 psiISO 178
Flexural Modulus 3.00 GPa435 ksiISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²2.38 ft-lb/in²ISO 180/1eA
Charpy Impact Unnotched NBNBISO 179/1eU
Charpy Impact, Notched 0.500 J/cm²2.38 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 60093
Dielectric Strength 25.0 kV/mm635 kV/inIEC 60243
Dissipation Factor 0.0300.030IEC 60250
Comparative Tracking Index 425 V425 VSolution B; IEC 60112
 525 V525 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 242 °C468 °FISO 11357
Oxygen Index 23 %23 %ISO 4589
Glow Wire Flammability Index 650 °C
@Thickness 1.60 mm
1200 °F
@Thickness 0.0630 in
ISO 60695-2-12
 
Processing PropertiesMetricEnglishComments
Feed Temperature 240 - 250 °C464 - 482 °F
Front Barrel Temperature 260 - 270 °C500 - 518 °F
Mold Temperature 60.0 - 80.0 °C140 - 176 °F
Drying Temperature 80.0 °C176 °F
Moisture Content <= 0.20 %<= 0.20 %
 
Descriptive Properties
Compression Zone250-260°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Domo TECHNYL® B 230 PA66/6, DRY
Domo TECHNYL® B 216 Natural D PA66/6, DRY
Domo TECHNYL® B 218 Black 21 N PA66/6, Conditioned
Domo TECHNYL® B 238 Black 21 N PA66/6, DRY
EMS-Grivory Grilon® TSZ 1 PA666

PRHOD737 / 137968

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.