MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Refractory Metals

CMW® ELKONITE® 10W53 Heat Treatable Copper Tungsten  (discontinued **)
Categories: Metal; Metal Matrix Composite; Nonferrous Metal; Refractory Metal; Tungsten Alloy

Material Notes: This material has been rebranded as a part of the NAECO® ELKON® product line.

Uses: Resistance / projection welding electrodes

Information provided by CMW Inc.

1

Vendors: PLANSEE SE: Whether it's high temperatures, aggressive chemicals or extreme mechanical loading: PLANSEE supplies a suitable product solution in refractory metals or composite materials. As the world market leader in powder metallurgically produced high performance materials we combine outstanding materials knowledge with profound applications and technology know-how. Visit us at www.plansee.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 14.79 g/cc0.5343 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 109109
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000616 ohm-cm0.00000616 ohm-cm(28% IACS)
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 150 W/m-K1040 BTU-in/hr-ft²-°F
Melting Point <= 3410 °C<= 6170 °F
Liquidus 3410 °C6170 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 24.11 %24.11 %
Nickel, Ni 0.69 %0.69 %
Silicon, Si 0.20 %0.20 %
Tungsten, W 75 %75 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CMW® ELKONITE® 2050C Copper Tungsten Contact Material ASTM B702, Class A, infiltrated
CMW® ELKONITE® 10W3 Copper Tungsten RWMA Class 11
CMW® ELKONITE® 1W3 Copper Tungsten RWMA Class 10
CMW® ELKONITE® 30W3 Infiltrated Copper Tungsten contact material ASTM B702, Class E, infiltrated, RWMA Class 12
NAECO® ELKON® R25 Copper Tungsten RWMA Class 11

NCMW30 / 15949

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.