MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil Santoprene® 691-73W175 Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Product Description: A soft, colorable thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for thin wall, architectural glazing and sealing applications. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for extrusion or thermoforming. It is polyolefin based and completely recyclable.

Key Features:

  • Recommended for glazing and sealing applications.
  • Designed for extruding thin sections with excellent definition (down to 0.33 mm [0.023"] radius) Long runs with minimal build-up of material on screen packs or narrow die sections.
  • Recommended for applications requiring excellent ozone resistance.
  • Recommended for applications requiring excellent flex fatigue resistance.
  • EU and China RoHS compliant.

Information provided by ExxonMobil Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.960 g/cc0.960 g/ccASTM D792 and ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 78782 mm; ISO 868
Tensile Strength at Break 8.30 MPa1200 psiAcross Flow; ASTM D412 and ISO 37
Tensile Stress at Strain 3.40 MPa
@Strain 100 %
493 psi
@Strain 100 %
Across Flow; ASTM D412 and ISO 37
Elongation at Break 470 %470 %Across Flow; ASTM D412 and ISO 37

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Santoprene® 291-75B150 Thermoplastic Vulcanizate
ExxonMobil Santoprene® 201-55 Thermoplastic Elastomer
ExxonMobil Santoprene® 251-80W232 Thermoplastic Elastomer
ExxonMobil Santoprene® 271-73 Thermoplastic Elastomer
ExxonMobil Santoprene® 9101-80E Thermoplastic Vulcanizate - Co-extrusion

PEXA920 / 125963

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.