MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Polykemi AB POLYfill PPC 200 E20 Polypropylene Copolymer, Elastomer Modified
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes:

Information provided by Polykemi AB

Key Words: Polypropylene Copolymer
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ISO 1183
Melt Index of Compound 20 g/10 min
@Load 2.16 kg,
Temperature 230 °C
20 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break <= 32.0 MPa<= 4640 psiISO/R527
Elongation at Yield 17 %17 %ISO/R527
Flexural Strength <= 28.0 MPa<= 4060 psiISO 178
Flexural Modulus 1.20 GPa
@Temperature 23.0 °C
174 ksi
@Temperature 73.4 °F
ISO 178
Charpy Impact, Notched  0.450 J/cm²
@Temperature -20.0 °C
2.14 ft-lb/in²
@Temperature -4.00 °F
ISO 179
 2.00 J/cm²
@Temperature 23.0 °C
9.52 ft-lb/in²
@Temperature 73.4 °F
ISO 179
 
Processing PropertiesMetricEnglishComments
Melt Temperature 180 - 230 °C356 - 446 °F
Mold Temperature 40.0 - 60.0 °C104 - 140 °F
Drying Temperature 70.0 - 80.0 °C158 - 176 °F
Dry Time 2 - 4 hour2 - 4 hourin circulation dryer
 2 - 4 hour2 - 4 hourin desiccant air dryer
Injection Pressure 40.0 - 70.0 MPa5800 - 10200 psi
Back Pressure 1.00 - 1.50 MPa145 - 218 psi
 
Descriptive Properties
Holding Pressure> 40% of injection pressure
Injection SpeedHighest possible

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total PPC 4524WZ Polypropylene, Impact Copolymer
Total PPC 4481WZ Polypropylene, Impact Copolymer
Teknor Apex Sarlink® 4490 Thermoplastic Elastomer
Teknor Apex Sarlink® 3480N Thermoplastic Elastomer
Teknor Apex Sarlink® 3439D Thermoplastic Elastomer

PPOLYK285 / 123010

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.