MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

LG Chemical SBR 1778 High Acrylonitrile Polymer
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Description: SBR 1778 is an oil extended cold polymerization SBR with 37.5 parts of discoloring paraffinic/naphthenic oil and light colored high molecular weight styrene-butadiene copolymer of 23.5% bound styrene. SBR 1778 combines the physical properties of oil extended polymers with the light color properties of naphthenic oil.

Applications: SBR 1778 can be used to hose, conveyor belt, tire and other industrial products for the light colored goods.

CAS No: 9003-55-8

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.920 g/cc0.920 g/cc
Volatiles 0.30 %0.30 %
Mooney Viscosity 46
@Temperature 100 °C
46
@Temperature 212 °F
ML 1+4
Ash 0.20 %0.20 %
 
Chemical PropertiesMetricEnglishComments
Styrene Content 23.5 %23.5 %Bound
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 22.6 MPa
@Treatment Temp. 145 °C,
Time 2100 sec
3280 psi
@Treatment Temp. 293 °F,
Time 0.583 hour
ASTM D412
Elongation at Break 500 %
@Treatment Temp. 145 °C,
Time 2100 sec
500 %
@Treatment Temp. 293 °F,
Time 0.583 hour
ASTM D412
300% Modulus 12.3 MPa
@Treatment Temp. 145 °C,
Time 2100 sec
1780 psi
@Treatment Temp. 293 °F,
Time 0.583 hour
ASTM D412
 
Descriptive Properties
ColorLight Tan Bale
ComponentsHAF68.75, ASTM D3185
 SBR 1739137.5, ASTM D3185
 Stearic Acid1, ASTM D3185
 Sulfur1.75, ASTM D3185
 TBBS1.38, ASTM D3185
 ZnO3, ASTM D3185
Oil Analysis27.3%
Organic Acid5%
Soap0.1%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Iran Petrochemical (PCC) Poliran SBR-1778 Styrene Butadiene Rubber

PLAY752 / 148762

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.