MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LNP VALOX® SMV5837 Polybutylene Terephthalate, 20% Glass Bead Reinforcement  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Glass Bead Filled

Material Notes: Will be VGB5820.

  • Forms: Pellets
  • Processing Method: Injection Molding
Information provided by LNP, a GE Plastics Company.

This data sheet is labeled Discontinued; however many LNP grades are still active under new names instituted after the SABIC purchase.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.46 g/cc1.46 g/ccASTM D792
Linear Mold Shrinkage 0.016 - 0.019 cm/cm
@Thickness 3.18 mm
0.016 - 0.019 in/in
@Thickness 0.125 in
ASTM D955
Linear Mold Shrinkage, Transverse 0.018 - 0.020 cm/cm
@Thickness 3.18 mm
0.018 - 0.020 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 40.7 MPa5900 psiType I, 5 mm/min; ASTM D638
 48.3 MPa7010 psiType I, 50 mm/min; ASTM D638
Tensile Strength, Yield 46.9 MPa6800 psiType I, 5 mm/min; ASTM D638
 51.7 MPa7500 psiType I, 50 mm/min; ASTM D638
Elongation at Break 16 %16 %Type I, 5 mm/min; ASTM D638
Flexural Yield Strength 93.1 MPa13500 psi(50.8 mm Span) 1mm/min; ASTM D790
Flexural Modulus 3.21 GPa466 ksi(50.8 mm Span) 1mm/min; ASTM D790
Izod Impact, Notched 0.320 J/cm0.599 ft-lb/inASTM D256
 3.60 J/cm6.74 ft-lb/inReverse; ASTM D256
Izod Impact, Unnotched 5.34 J/cm10.0 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear  65.0 µm/m-°C
@Temperature -40.0 - 38.0 °C
36.1 µin/in-°F
@Temperature -40.0 - 100 °F
ASTM D696
 140 µm/m-°C
@Temperature 60.0 - 138 °C
77.8 µin/in-°F
@Temperature 140 - 280 °F
ASTM D696
CTE, linear, Transverse to Flow  68.0 µm/m-°C
@Temperature -40.0 - 38.0 °C
37.8 µin/in-°F
@Temperature -40.0 - 100 °F
ASTM D696
 150 µm/m-°C
@Temperature 60.0 - 138 °C
83.3 µin/in-°F
@Temperature 140 - 280 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
@Thickness 6.35 mm
158 °F
@Thickness 0.250 in
Unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 243 - 254 °C469 - 489 °F
Middle Barrel Temperature 249 - 260 °C480 - 500 °F
Front Barrel Temperature 254 - 266 °C489 - 511 °F
Nozzle Temperature 254 - 271 °C489 - 520 °F
Melt Temperature 254 - 277 °C489 - 531 °F
Mold Temperature 65.6 - 93.3 °C150 - 200 °F
Drying Temperature 121 °C250 °F
Dry Time 3 - 12 hour3 - 12 hour
Moisture Content 0.020 %0.020 %Suggested
Back Pressure 0.345 - 0.689 MPa50.0 - 99.9 psi
Clamp Pressure 41.0 - 83.0 MPa5950 - 12000 psi
Shot Size 40 - 80 %40 - 80 %Suggested
Vent Depth 0.00250 - 0.00380 cm0.000984 - 0.00150 in
Screw Speed 50 - 80 rpm50 - 80 rpm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Techmer ES Elastoblend® PA6/6 GF13 IM HS BK 13% Glass Filled
Saint-Gobain Quartzel® Fiber/Epoxy Resin Unidirectional Composite
LNP Thermocomp® MB-1006 HS BK8-115 Polypropylene, Glass Bead
LNP Lexan® SML5750 Polycarbonate, 50% Glass Bead / Glass Fiber Reinforced
LNP Lexan® SML5704 Polycarbonate, 50% Glass Bead / Glass Fiber Reinforced

PZLNP1583 / 51665

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.