MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SK Chemicals SKYTHANE® S385A Polyester Based Thermoplastic Polyurethane Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Polyester Grade

Material Notes: Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:
  • Keyboard Covers
  • Outsoles of Soccer Shoes
  • Wire and Cable
  • Airbags
  • Sheets and Film
  • Hoses and Tubing
  • Shoe Components
  • Fire Hoses

Information provided by SK Chemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/ccASTM D792
Linear Mold Shrinkage 0.0045 cm/cm0.0045 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8585ASTM D2240
Hardness, Shore D 3535ASTM D2240
Tensile Strength, Ultimate 34.3 MPa4980 psiASTM D412
Elongation at Break 810 %810 %ASTM D412
100% Modulus 4.34 MPa
@Strain 100 %
630 psi
@Strain 100 %
ASTM D412
300% Modulus 8.791 MPa
@Strain 300 %
1275 psi
@Strain 300 %
ASTM D412
Resilience 3030Vertical Rebound; ASTM D2632
Tear Strength 93.2 kN/m532 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 1313H18 wheel, 1000g load; ASTM D1044
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 62.0 °C144 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Processing Temperature 190 °C374 °FTransition Temperature
 190 °C374 °FMetering Temperature
Middle Barrel Temperature 185 °C365 °F
Nozzle Temperature 195 °C383 °F
Zone 1 175 °C347 °F
Zone 2 180 °C356 °F
Zone 3 185 °C365 °F
Zone 4 190 °C374 °F
Adapter Temperature 190 °C374 °F
Die Temperature 190 °C374 °FTip
 195 °C383 °FBody
Mold Temperature 20.0 - 40.0 °C68.0 - 104 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Huntsman IROGRAN® A 98 E 4066 Polyester-Based TPU-High Performance Grade
Dow SE SLR-4610 Solution polymerized Styrene Butadiene Rubber (S-SBR)
Denka REOMER G G8082 Thermoplastic Elastomer, For Injection Molding
Celanese Riteflex® 677 TPC, Unfilled
Celanese Riteflex® 663 TPC, Unfilled

PSK020 / 67755

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.