MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mitsubishi Xantar® RX 2124 Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: A versatile thermoplastic resin that is suitable for a wide range of applications and can be converted using all common melt-processing techniques.

Information provided by Mitsubishi Engineering Plastics Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³
Melt Density 1.01 g/cc
@Temperature 300 °C
0.0365 lb/in³
@Temperature 572 °F
Water Absorption 0.35 %0.35 %
Viscosity Number 50 cm³/g0.50 dl/gLimiting Viscosity Number
 50 cm³/g0.50 dl/g
Linear Mold Shrinkage, Flow 0.0060 cm/cm0.0060 in/in
Melt Flow 10 g/10 min
@Load 1.20 kg,
Temperature 300 °C
10 g/10 min
@Load 2.65 lb,
Temperature 572 °F
cm³/10 min Volumetric Rate
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 60.0 MPa8700 psi
Elongation at Break >= 50 %>= 50 %
Elongation at Yield 6.0 %6.0 %
Tensile Modulus 2.30 GPa334 ksi
Flexural Strength 90.0 MPa13100 psi
Flexural Modulus 2.40 GPa348 ksi
Izod Impact, Notched (ISO) 80.0 kJ/m²38.1 ft-lb/in²
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cm
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohm
Dielectric Constant  2.9
@Frequency 1e+6 Hz
2.9
@Frequency 1e+6 Hz
 3.0
@Frequency 100 Hz
3.0
@Frequency 100 Hz
Dielectric Strength 29.0 kV/mm737 kV/in
Dissipation Factor  0.00066
@Frequency 100 Hz
0.00066
@Frequency 100 Hz
 0.0092
@Frequency 1e+6 Hz
0.0092
@Frequency 1e+6 Hz
Comparative Tracking Index 225 V225 V
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 65.0 µm/m-°C36.1 µin/in-°F
Specific Heat Capacity 1.71 J/g-°C0.409 BTU/lb-°Fmelt
Thermal Conductivity 0.240 W/m-K1.67 BTU-in/hr-ft²-°Fmelt
Hot Ball Pressure Test 125 °C257 °F
Deflection Temperature at 1.8 MPa (264 psi) 130 °C266 °F
Vicat Softening Point 148 °C
@Load 5.10 kg
298 °F
@Load 11.2 lb
rate 50°C/h
Flammability, UL94 V-0
@Thickness 2.00 mm
V-0
@Thickness 0.0787 in
Oxygen Index 35 %35 %
Glow Wire Ignition Temperature  850 °C
@Thickness 1.50 mm
1560 °F
@Thickness 0.0591 in
 850 °C
@Thickness 3.00 mm
1560 °F
@Thickness 0.118 in
Glow Wire Flammability Index  960 °C
@Thickness 1.50 mm
1760 °F
@Thickness 0.0591 in
 960 °C
@Thickness 3.00 mm
1760 °F
@Thickness 0.118 in
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 89 %89 %
 
Processing PropertiesMetricEnglishComments
Melt Temperature 300 °C572 °FAs Tested; Injection
Mold Temperature 90.0 °C194 °FAs Tested; Injection
Ejection Temperature 131 °C268 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Xantar® G2F 23 R Polycarbonate-10% Glass Reinforced
Covestro Makrolon® 6557 Polycarbonate, Injection Grade
Westlake Plastics Zelux® W Window Grade Polycarbonate
Samyang Trirex® PC-3020HF 22 MFI Clear Polycarbonate
Overview of materials for PVC, Molded

PMITSU9312 / 191986

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.