MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Carpenter Micro-Melt® M-42 Alloy (AISI M42)
Categories: Metal; Ferrous Metal; Tool Steel

Material Notes: Micro-Melt® M-42 alloy is a powder metal super-high-speed steel possessing a hardness capability of Rockwell C 68/70. This alloy has been used for cutting tools in the toughest machining operations. The advantages of Micro-Melt premium high speed steels include ease of grinding, response to heat treatment, more uniform structure, greater wear resistance and improved toughness. In addition, Carpenter's unique hot rolling and rotary forging capabilities impart minimal distortion characteristics to these alloys.

Applications: Twist drills, Turning tools, End mills, Milling cutters, Broaches, Router Bits, Form tools, Keyway cutters, Dovetail tools, Flycutters, Thread rolling dies, Tool bits

Information provided by Carpenter Technology Corporation.

Micro-Melt® is a registered trademark of Carpenter Technology Corporation.

Key Words: UNS T11342
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 7.98 g/cc7.98 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 64 - 6664 - 66As quenched
 65 - 6765 - 67Tempered at 1100°F
Modulus of Elasticity 206.8 GPa29990 ksi
Izod Impact Unnotched 14.9 - 31.2 J11.0 - 23.0 ft-lb
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 1.1 %1.1 %
Chromium, Cr 3.75 %3.75 %
Cobalt, Co 8.25 %8.25 %
Iron, Fe 74.69 %74.69 %As Balance
Molybdenum, Mo 9.5 %9.5 %
Sulfur, S 0.060 %0.060 %
Tungsten, W 1.5 %1.5 %
Vanadium, V 1.15 %1.15 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type M42 Molybdenum High Speed Tool Steel (UNS T11342)
Crucible Steel REX® M42 High Speed Steel, AISI M42
PSM Industries Pacific Sintered Metals FCC-214-S(HT) High Carbon Copper Steel Powdered Metal (MPIF FC-0208-80HT)
Latrobe Dynamax™ ASTM M42, DIN 1.3247 Super High Speed Steel
Carpenter Micro-Melt® T-15 Alloy (AISI T15)

NCARN10 / 15849

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.