MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Akro-Plastic Akromid® B3 GK 15 natural PA6, Dry, 15% Glass Bead Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass Bead Filled

Material Notes: Description: AKROMID B3 GK 15 natural is a 15% glass bead filled polyamide 6 with low warpage, high surface finish and light inherent color

Applications: Applications are housings and covers in the automotive-, electro- and furniture industry

Information provided by Akro-Plastic GmbH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 g/cc0.0444 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 85.0 MPa12300 psi5 [mm/min]; ISO 527-2
Elongation at Break 4.5 %4.5 %5 [mm/min]; ISO 527-2
Tensile Modulus 4.00 GPa580 ksi1 [mm/min]; ISO 527-2
Flexural Strength 125 MPa18100 psi2 [mm/min]; ISO 178
Flexural Modulus 3.60 GPa522 ksi2 [mm/min]; ISO 178
Flexural Strain at Break 6.0 %6.0 %2 mm/min; ISO 178
Charpy Impact Unnotched  3.00 J/cm²
@Temperature 23.0 °C
14.3 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
 3.50 J/cm²
@Temperature -30.0 °C
16.7 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched  0.250 J/cm²
@Temperature 23.0 °C
1.19 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 0.270 J/cm²
@Temperature -30.0 °C
1.28 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 222 °C432 °FDSC, 10K/min; DIN EN 11357-1
Deflection Temperature at 0.46 MPa (66 psi) 186 °C367 °FISO 75/B
Deflection Temperature at 1.8 MPa (264 psi) 67.0 °C153 °FISO 75/A
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman SCHULAMID® 6 GF15H 15% Glass Bead Reinforced, Heat Stabilized Nylon 6
Techmer ES HiFill® PA6 GB15 L BK 15% Glass Bead Filled
BASF Ultramid® B3EG3 BK00564 15% Glass Filled PA6 (Dry)
Akro-Plastic Akromid® B3 GK 15 natural PA6, Conditioned, 15% Glass Bead Filled
Ravago Manufacturing Americas Hylon N2030GBHL Nylon 6, 30% Glass Beads, DAM

PAKRO408 / 182995

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.