MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay VTS263
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: VTS263 is an epoxy syntactic core film capable of initially curing at temperatures between 65 and 120°C (149 and 248°F). It has been formulated to co-cure with VTM®260 series of prepreg matrices. VTS263 can be used for edge filling large sandwich panels or as the core for thin and variable depth sandwich construction components.

Features & Benefits:

  • 30 days out life at 21°C (70°F)
  • 12 months storage at -18°C (0°F)
  • Flexible cure capability
  • Service temperature up to 120°C (248°F)

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.800 g/cc0.0289 lb/in³Cured @: 1 hr, 120°C, 15 psi
Storage Temperature -18.0 °C-0.400 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 120 °C248 °F
Glass Transition Temp, Tg 115 °C239 °FDMA E' onset, Post-cure: 30 mins at 120°C
 
Processing PropertiesMetricEnglishComments
Cure Time  30.0 min
@Temperature 120 °C
0.500 hour
@Temperature 248 °F
 120 min
@Temperature 100 °C
2.00 hour
@Temperature 212 °F
 480 min
@Temperature 80.0 °C
8.00 hour
@Temperature 176 °F
Shelf Life 12.0 Month12.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay VTA® 266 Film
Solvay VTF 261 Film

PCYTED103 / 180405

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.