MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Geon® Performance Solutions Vinyl Rigid Molding M5240 Natural Polyvinyl Chloride, Rigid
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade

Material Notes:

NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of unpigmented compounds or so-called natural compounds generally is inferior to pigmented compounds. Unpigmented weatherable compounds may also contain non-pigment ingredients which can interact unpredictably with pigments to produce unexpected weathering results. Therefore, in applications where processors or customers would like to use an unpigmented compound, or add their own pigment package, it is the customer's responsibility to determine whether or not the weathering performance after pigmenting is acceptable in their specific end-use application.

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.34 g/cc1.34 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0020 - 0.0050 cm/cm0.0020 - 0.0050 in/inASTM D955
Spiral Flow 61.0 cm24.0 in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7979ASTM D2240
Tensile Strength, Yield 42.7 MPa6190 psi51 mm/min; ASTM D638
Elongation at Break 45 %45 %51 mm/min; ASTM D638
Tensile Modulus 2.34 GPa339 ksi51 mm/min; ASTM D638
Flexural Strength 71.0 MPa10300 psiASTM D790
Flexural Modulus 2.41 GPa350 ksiASTM D790
Izod Impact, Notched  1.60 J/cm
@Thickness 3.18 mm,
Temperature -18.0 °C
3.00 ft-lb/in
@Thickness 0.125 in,
Temperature -0.400 °F
Injection Molded; ASTM D256A
 3.70 J/cm
@Thickness 3.18 mm,
Temperature 0.000 °C
6.93 ft-lb/in
@Thickness 0.125 in,
Temperature 32.0 °F
Injection Molded; ASTM D256A
 7.50 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
14.1 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi)  72.8 °C
@Thickness 6.35 mm
163 °F
@Thickness 0.250 in
Unannealed; ASTM D648
 77.8 °C
@Thickness 6.35 mm
172 °F
@Thickness 0.250 in
Annealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)  71.1 °C
@Thickness 6.35 mm
160 °F
@Thickness 0.250 in
Unannealed; ASTM D648
 76.1 °C
@Thickness 6.35 mm
169 °F
@Thickness 0.250 in
Annealed; ASTM D648
UL RTI, Electrical 90.0 °C194 °FUL 746
UL RTI, Mechanical with Impact 85.0 °C185 °FUL 746
UL RTI, Mechanical without Impact 90.0 °C194 °FUL 746
Flammability, UL94  V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
ALL; UL 94
 5VA
@Thickness 1.60 mm
5VA
@Thickness 0.0630 in
ALL; UL 94
 
Processing PropertiesMetricEnglishComments
Melt Temperature 199 - 210 °C390 - 410 °F
 
Descriptive Properties
FeaturesGeneral Purpose
 High Impact Resistance
 Medium Flow
FormsPellets
Generic MaterialPVC, Rigid
Generic NamePolyvinyl Chloride, Rigid (PVC, Rigid)
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesConstruction Applications
 General Purpose
 Outdoor Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Geon® Performance Solutions Vinyl Rigid Molding M5240 Polyvinyl Chloride, Rigid
Geon® Performance Solutions Vinyl Rigid Molding 6957 Polyvinyl Chloride, Rigid
Avient Novablend™ 6602 Polyvinyl Chloride, Rigid
Geon® Performance Solutions Vinyl Rigid Molding M4825 Polyvinyl Chloride, Rigid
Geon® Performance Solutions Vinyl Rigid Molding M3800 Polyvinyl Chloride, Rigid

PH0POL0430 / 144999

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.