MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Envalior Durethan® DP BM 65 X FM30 901510 Nylon 6 (PA6), 65% Mineral/Glass Fiber Reinforced, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass/Mineral Reinforced

Material Notes: PA 6, 65% mineral/glass fibers, injection molding, halogen free flame retardant, improved flowability despite the high degree of filling

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.69 g/cc0.0611 lb/in³ISO 1183
Moisture Absorption at Equilibrium 1.2 %1.2 %50% RH; ISO 62
Water Absorption at Saturation 3.5 %3.5 %IOS 62
Linear Mold Shrinkage, Flow 0.0040 cm/cm0.0040 in/in60x60x2; 280 °C / MT 80°C; 500 bar; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0050 cm/cm0.0050 in/in60x60x2; 280 °C / MT 80°C; 500 bar; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 175 MPa25400 psi5 mm/min; ISO 527-1,-2
Elongation at Break 1.6 %1.6 %5 mm/min; ISO 527-1,-2
Tensile Modulus 12.1 GPa1750 ksi1 mm/min; ISO 527-1,-2
Flexural Strength 175 MPa25400 psi2 mm/min; ISO 178-A
Flexural Modulus 12.3 GPa1780 ksi2 mm/min; ISO 178-A
Flexural Strain at Break 1.8 %1.8 %2 mm/min; ISO 178-A
Izod Impact, Notched (ISO) <= 10.0 kJ/m²<= 4.76 ft-lb/in²ISO 180-1A
Izod Impact, Unnotched (ISO) 25.0 kJ/m²11.9 ft-lb/in²ISO 180-1U
Charpy Impact Unnotched 2.50 J/cm²11.9 ft-lb/in²ISO 179-1eU
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 26.3 kV/mm
@Thickness 1.00 mm
668 kV/in
@Thickness 0.0394 in
IEC 60243-1
Comparative Tracking Index 600 V600 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 30.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
16.7 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
CTE, linear, Transverse to Flow 50.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
27.8 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Melting Point 220 °C428 °F10°C/min; ISO 11357-1,-3
Deflection Temperature at 0.46 MPa (66 psi) 200 °C392 °FISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 181 °C358 °FISO 75-1,-2
Vicat Softening Point 204 °C
@Load 5.10 kg
399 °F
@Load 11.2 lb
120°C/h; ISO 306
Flammability, UL94  V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 V-0
@Thickness 1.20 mm
V-0
@Thickness 0.0472 in
Oxygen Index 49.1 %49.1 %Method A; ISO 4589-2
Glow Wire Ignition Temperature 775 °C
@Thickness 0.800 mm
1430 °F
@Thickness 0.0315 in
IEC 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 0.800 mm
1760 °F
@Thickness 0.0315 in
IEC 60695-2-12
Shrinkage, MD 0.10 %
@Treatment Temp. 120 °C,
Time 14400 sec
0.10 %
@Treatment Temp. 248 °F,
Time 4.00 hour
Post-Shrinkage Flow Direction; 60x60x2; ISO 294-4
Shrinkage, TD 0.10 %
@Treatment Temp. 120 °C,
Time 14400 sec
0.10 %
@Treatment Temp. 248 °F,
Time 4.00 hour
60x60x2; ISO 294-4
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 °C500 °Finjection molding
 250 - 280 °C482 - 536 °F
Mold Temperature 80.0 °C176 °Finjection molding
 80.0 - 100 °C176 - 212 °F
Drying Temperature 80.0 °C176 °F
Dry Time 2.00 - 6.00 hour2.00 - 6.00 hour
Moisture Content 0.030 - 0.070 %0.030 - 0.070 %Karl Fischer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Durethan® DP BM 65 X FM30 901510 Nylon 6 (PA6), 65% Mineral/Glass Fiber Reinforced, Conditioned
LATI Latamid 6 H2 G/65 PA 6, 65% Glass Fiber Reinforced, Heat Stabilized
Envalior Durethan® KU 2-2184/15 H3.0 000000 Nylon 6 (PA6), 65% Glass/Mineral Reinforced, Flame Retardant, Conditioned
Plastcom SLOVAMID 6 GF 65 PA6, 65% glass fibre
Envalior Durethan® BG 60 X XF 900116 Nylon 6 (PA6), 60% Glass Fiber/Glass spheres Reinforced, Dry

PLANW9492 / 208364

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.