MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Teknor Apex Chemlon® 125-15 MGH Nylon 66, 25% Mineral Reinforced, 15% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: Notes: 25% Mineral - 15% Glass; Excellent stiffness and strength, especially at high temperatures, with improved warpage control over glass reinforced products; FMVSS Flammability: Passes, FMVSS 302

Features: Heat Stabilized

Processing Method: Injection Method

Forms: Pellets

Automotive Specifications: Chrysler Ms-DB41 CPN2554 Color: BK001 Black

Information Provided by Teknor Apex

Key Words: Polyamide 66
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.54 g/cc1.54 g/ccASTM D792
Linear Mold Shrinkage 0.0015 - 0.0040 cm/cm0.0015 - 0.0040 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 128 MPa18500 psiASTM D638
Elongation at Break 2.5 %2.5 %ASTM D638
Elongation at Yield 2.5 %2.5 %ASTM D638
Flexural Strength 190 MPa27500 psiASTM D790
Flexural Modulus 7.93 GPa1150 ksiASTM D790
Izod Impact, Notched 0.747 J/cm
@Temperature 22.8 °C
1.40 ft-lb/in
@Temperature 73.0 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 550 V550 VUL 746
 
Thermal PropertiesMetricEnglishComments
Melting Point 257 °C495 °FDSC
Deflection Temperature at 1.8 MPa (264 psi) 241 °C465 °FUnannealed; ASTM D648
UL RTI, Electrical 65.0 °C
@Thickness 0.749 mm
149 °F
@Thickness 0.0295 in
UL 746
UL RTI, Mechanical with Impact 65.0 °C
@Thickness 0.749 mm
149 °F
@Thickness 0.0295 in
UL 746
UL RTI, Mechanical without Impact 65.0 °C
@Thickness 0.749 mm
149 °F
@Thickness 0.0295 in
UL 746
Flammability, UL94 HB
@Thickness 0.749 mm
HB
@Thickness 0.0295 in
Oxygen Index 24 %24 %ASTM D2863
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 241 - 257 °C465 - 495 °F
Middle Barrel Temperature 263 - 279 °C505 - 535 °F
Front Barrel Temperature 268 - 285 °C515 - 545 °F
Nozzle Temperature 268 - 282 °C515 - 540 °F
Melt Temperature 263 - 285 °C505 - 545 °FProcessing Temperature
Drying Temperature 79.4 °C175 °F
Moisture Content 0.20 %0.20 %
 
Descriptive Properties
Suggested Regrind, max25

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wellman Wellamid® MRGF25/15 42H-N 25% Mineral/15% Glass Fiber Reinforced Nylon 6, Heat Stabilized
Teknor Apex Chemlon 225-15 MG Nylon 6, 25% Mineral/15% Glass Fiber Reinforced
Teknor Apex Chemlon 125-15 MG Nylon 66, 25% Mineral/15% Glass Fiber Reinforced
RTP Company RTP PA66 15 GF 25 M BLK Nylon 6/6 (PA), Value Product - 15% Glass Fiber - 25% Mineral - Heat Stabilized
Envalior Akulon® K224-HGM35 (Dry) 15% Glass Reinforced, 25% Mineral Reinforced, Heat Stabilized Nylon 6 (North America)

PTEKNO435 / 128612

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.