QGel 310 is a clear, very soft, tough moderately cross-linked silicone polymer. Silicone gels are used to provide protection from vibration and thermal or mechanical shock. Silicone gels also provide excellent moisture protection. Key Features: - 24 hour room temperature or heat cure
- One to one mix ratio
- Soft but resilient
- Dispensing equipment not necessary
Part of the Amber Chemical Group. Data provided by manufacturer.Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017 |