MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DSM Fibre Intermediates Nyrim® 1525 (Glass), Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is processed via Reaction Injection Moulding (RIM) technology. Nyrim® is a registered trademark.

Information provided by the manufacturer, Brueggemann Chemical.

Key Words: RIM materials
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.322 g/cc0.04776 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8282ISO 868
Tensile Strength, Ultimate 55.0 MPa7980 psiISO 527
Elongation at Break 7.0 %7.0 %ISO 527
Modulus of Elasticity 3.75 GPa544 ksiISO 527
Flexural Modulus 3.85 GPa558 ksiISO 178
Izod Impact, Notched (ISO) 9.00 kJ/m²4.28 ft-lb/in²ISO 180
Charpy Impact, Notched 0.600 J/cm²2.86 ft-lb/in²DIN 53453
 0.500 J/cm²
@Temperature -40.0 °C
2.38 ft-lb/in²
@Temperature -40.0 °F
DIN 53453

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
SK Chemicals SKYPEL G182D General Grade
Brueggemann Chemical Nyrim® 1000 (Dry)
Chengdu Polyster H9275Y Thermoplastic Polyether-ester Elastomer (TPEE)
Chosun Refractories SSB-1 Bricks, Reaction Bonded SiC
Chosun Refractories SBSN Bricks, Reaction Bonded SiC

PDSMN090 / 31487

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.